MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petromont 3101 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petromont HDPE 3101 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is intended for a broad range of injection moulding applications including open-head pails, housewares, toys and food containers.

Petromont HDPE 3101 is a low molecular weight hexene modified copolymer resin with a very narrow molecular weight distribution. The resin has been especially designed for use in injection moulding applications where thin-walled parts having excellent toughness and gloss, combined with superior flow characteristics, are required.

Key Words: Food Grade
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D1505
ESCR 10% Igepal® 50 hour50 hourF50; ASTM D1693
Melt Flow 20 g/10 min20 g/10 minI2; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.9 MPa4190 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus 1.20 GPa174 ksiASTM D790
Tensile Impact Strength 67.3 kJ/m²32.0 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -100 °C<= -148 °FASTM D746
 
Descriptive Properties
ProcessInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 92 E 5670 FCM Ester-Based TPU-For Food Contact
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE)
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE)
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE)

PPETROM14 / 56208

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.