MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 92 E 5670 FCM Ester-Based TPU-For Food Contact
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Introduction: IROGRAN A 92 E 5670 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a specially designed, flexible material with a broad processing window. IROGRAN A 92 E 5670 FCM is a food contact material.

Performance Features:

  • High oil resistance
  • High production rate
  • Good melt flow
  • Easy coloring
  • Complies with FDA CFR 175.105 / 177.2600
Applications:
  • Cable jacketing
  • Tubing
  • Technical extrusion

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASDTM D792
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
Melt Index of Compound 62 g/10 min
@Load 10.0 kg,
Temperature 190 °C
62 g/10 min
@Load 22.0 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
Hardness, Shore D 3838ASTM D2240
Tensile Strength at Break 40.0 MPa5800 psiDIN 53504
Elongation at Break 570 %570 %DIN 53504
Compression Set  25 %
@Temperature 23.0 °C,
Time 86400 sec
25 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D395
 40 %
@Temperature 70.0 °C,
Time 86400 sec
40 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Feed Temperature 195 °C383 °F
Front Barrel Temperature 205 °C401 °F
Adapter Temperature 210 °C410 °F
Die Temperature 210 °C410 °F
Roll Temperature 170 - 190 °C338 - 374 °FFront, 32 rpm
 170 - 190 °C338 - 374 °FRear, 27 rpm
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
Huntsman IROGRAN® A 85 P 4394 FCM Ether-Based TPU-For Food Contact
Petromont 3101 High Density Polyethylene Resin
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether
Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact

PHU9940 / 150400

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.