MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec Rubalit® A 1898 Alumina, 98%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond of high strength is achieved. Rubalit® A 1898 has high dielectric strength and volume resistivity combined with good thermal conductivity. The metallization system consists of tungsten overplated with nickel for effective hard solder wetting properties. For soft soldering purposes, an additional tin layer can be applied. The use of special brazing materials (e.g., AgCu solder) assures a reliable interface during processing and handling. Brazing is performed in an inert gas atmosphere or vacuum, using temperature/time profiles specifically adapted for each product. The result is a vacuum-tight ceramic-to-metal joint with high bond strength. Glazes can be optionally applied to each product in order to prevent contamination of the ceramic surface, which helps preserve the ceramic's insulating properties under operating conditions.

Key Words: Al2O3, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.80 g/cc0.137 lb/in³
Water Absorption 0.00 %0.00 %
Permeability 0.000.00%, Gas
Weibull Modulus 1111
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 14001400HV 10
Modulus of Elasticity 350 GPa50800 ksi
Flexural Strength 400 MPa58000 psi
Compressive Strength 3800 MPa551000 psi
Poissons Ratio 0.220.22
Fracture Toughness 4.10 MPa-m½3.73 ksi-in½KIC
Shear Modulus 143 GPa20700 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 1.00e+7 ohm-cm
@Temperature 800 °C
>= 1.00e+7 ohm-cm
@Temperature 1470 °F
 >= 1.00e+11 ohm-cm
@Temperature 400 °C
>= 1.00e+11 ohm-cm
@Temperature 752 °F
 >= 1.00e+14 ohm-cm
@Temperature 20.0 °C
>= 1.00e+14 ohm-cm
@Temperature 68.0 °F
Dielectric Constant 10
@Frequency 1e+7 Hz
10
@Frequency 1e+7 Hz
Dielectric Strength 25.0 kV/mm635 kV/in
Dissipation Factor 0.0010
@Frequency 1e+7 Hz
0.0010
@Frequency 1e+7 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.40 µm/m-°C
@Temperature 20.0 - 200 °C
3.00 µin/in-°F
@Temperature 68.0 - 392 °F
 6.90 µm/m-°C
@Temperature 20.0 - 400 °C
3.83 µin/in-°F
@Temperature 68.0 - 752 °F
 7.70 µm/m-°C
@Temperature 20.0 - 600 °C
4.28 µin/in-°F
@Temperature 68.0 - 1110 °F
 8.50 µm/m-°C
@Temperature 20.0 - 1000 °C
4.72 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.900 J/g-°C
@Temperature 20.0 - 100 °C
0.215 BTU/lb-°F
@Temperature 68.0 - 212 °F
Average
Thermal Conductivity 26.0 W/m-K
@Temperature 20.0 - 100 °C
180 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 98 %98 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Rubalit® A 1894 Alumina, 94%
CeramTec 965 Toughened Alumina (Al2O3-ZrO2)
CeramTec 433 Alumina, 99.9%
CeramTec 614/698 Alumina, 96%
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2

CCERA956 / 107556

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.