MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Gravi-Tech™ GRV-NJ-110-W Polyamide 12 (Nylon 12)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 11.0 g/cc11.0 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 44.8 MPa6500 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 1.0 %1.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 8.96 GPa1300 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 68.9 MPa9990 psiASTM D790
Flexural Modulus 8.27 GPa1200 ksiASTM D790
Izod Impact, Notched 0.800 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.50 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
@Thickness 6.35 mm
311 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 288 °C500 - 550 °F
Mold Temperature 82.2 - 149 °C180 - 300 °F
Drying Temperature 79.4 °C175 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
FeaturesHigh Density
 Non-Toxic
FormsPellets
Generic MaterialNylon 12
Generic NamePolyamide 12 (Nylon 12)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesIndustrial Applications
 Medical/Healthcare Applications
 Projectiles
 Radiation Shielding
 Sporting Goods
 Weighting & Balancing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 299 A X 108950 J Nylon 6 (PA), High Gravity Compound - Non Magnetic
RTP Company RTP 299 A X 92682 J Nylon 6 (PA), High Gravity Compound
EMS-Grivory Grilamid® L 25 nat PA12 Film Grade
Overview of materials for Polyetherimide (PEI)
RTP Company RTP 2100 Polyetherimide (PEI)

PH0POL0638 / 145207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.