BASF Ultraform® N2720 M63 30% Mineral Filled POM
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Copolymer, Mineral Filled
Material Notes:
Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.650
-
0.900
g/cc
0.0235
-
0.0325
lb/in³
Density
1.65
g/cc
0.0596
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
0.15 %
0.15 %
23°C; 50% RH; ISO 62
Water Absorption at Saturation
0.90 %
0.90 %
ISO 62
Linear Mold Shrinkage, Flow
0.012
cm/cm
0.012
in/in
ISO 2577
Linear Mold Shrinkage, Transverse
0.015
cm/cm
0.015
in/in
ISO 2577
Melt Flow
6.27
g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.27
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
190
MPa
@Load 98.0 kg,
Time 30.0 sec
27600
psi
@Load 216 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield
75.0
MPa
10900
psi
50 mm/min; ISO 527-2
Elongation at Break
6.0 %
6.0 %
Nominal, 50mm/min; ISO 527-2
Elongation at Yield
5.0 %
5.0 %
ISO 527-2
Modulus of Elasticity
7.00
GPa
1020
ksi
ISO 527-2
Izod Impact, Notched (ISO)
3.50
kJ/m²
@Temperature -30.0 °C
1.67
ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
3.50
kJ/m²
@Temperature 23.0 °C
1.67
ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched
5.50
J/cm²
@Temperature -30.0 °C
26.2
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
5.50
J/cm²
@Temperature 23.0 °C
26.2
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.300
J/cm²
@Temperature -30.0 °C
1.43
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
0.350
J/cm²
@Temperature 23.0 °C
1.67
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours
2750
MPa
@Strain <=0.5 %
399000
psi
@Strain <=0.5 %
ISO 899-1
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+12
ohm-cm
1.00e+12
ohm-cm
IEC 60093
Surface Resistance
1.00e+14
ohm
1.00e+14
ohm
IEC 60093
Dielectric Constant
4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
43.0
kV/mm
1090
kV/in
IEC 60243-1
Dissipation Factor
0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index
600
V
600
V
Test solution A; IEC 60112
600
V
600
V
Test solution B; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
45.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
25.0
µin/in-°F
@Temperature 73.4 - 131 °F
DIN 53752
Melting Point
166
°C
331
°F
DIN 53765
Maximum Service Temperature, Air
110
°C
230
°F
Deflection Temperature at 1.8 MPa (264 psi)
140
°C
284
°F
ISO 75-2
Vicat Softening Point
155
°C
311
°F
ISO 306
Decomposition Temperature
>=
240
°C
>=
464
°F
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Ignition Temperature
320
-
340
°C
608
-
644
°F
ASTM D1929
Processing Properties
Metric
English
Comments
Processing Temperature
200
°C
392
°F
Hopper Throat
Zone 1
205
°C
401
°F
Feed zone
Zone 2
205
°C
401
°F
Compression
Zone 3
210
°C
410
°F
Metering-zone
Zone 4
210
°C
410
°F
Nozzle
Melt Temperature
190
-
230
°C
374
-
446
°F
Injection-molding
210
°C
410
°F
Optimal
Mold Temperature
60.0
-
120
°C
140
-
248
°F
Injection-molding
100
°C
212
°F
Optimal
Drying Temperature
100
°C
212
°F
Dry Time
3
hour
3
hour
Descriptive Properties
Commercial Status
Europe
Peripheral Screw Speed
<0.3 m/s
Primary Processing Technique
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultraform® N 2200 G53 UNC Q600 25% Glass Filled POM
BASF Ultraform® H 2320 006 Q600 POM
BASF Ultraform® N 2640 Z4 UNC Q600 POM
KEP Kepital® TC3020 Acetal Copolymer, Talc Filled
BASF Ultraform® N2200 G43 POM
PBASG0143 / 131776
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.