MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultraform® N 2640 Z4 UNC Q600 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Water Absorption 0.80 %0.80 %ISO 62
Moisture Absorption at Equilibrium 0.25 %0.25 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.019 cm/cm0.019 in/inASTM Data; MD
Linear Mold Shrinkage, Flow 0.018 cm/cm0.018 in/inISO Data
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inISO Data
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 44.0 MPa6380 psi50mm/min; ISO 527
 44.0 MPa6380 psi2 in/min; ASTM Test
 22.0 MPa
@Temperature 80.0 °C
3190 psi
@Temperature 176 °F
ISO Data
Elongation at Break >= 50 %>= 50 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 14 %14 %50mm/min; ISO 527
 14 %14 %2 in/min; ASTM Test
 17 %
@Temperature 80.0 °C
17 %
@Temperature 176 °F
ISO Data
Tensile Modulus 1.66 GPa241 ksiASTM Test
 1.70 GPa247 ksi1mm/min; ISO 527
Flexural Modulus 1.66 GPa241 ksiASTM Test
Izod Impact, Notched 0.907 J/cm
@Temperature -40.0 °C
1.70 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 1.49 J/cm
@Thickness 3.17 mm
2.79 ft-lb/in
@Thickness 0.125 in
ASTM Test
Charpy Impact Unnotched NBNBISO 179
 30.0 J/cm²
@Temperature -30.0 °C
143 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Tensile Creep Modulus, 1 hour 1350 MPa196000 psiISO 899
Tensile Creep Modulus, 1000 hours 1000 MPa145000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
IEC 60250
 4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm1020 kV/inIEC 60243-1
Dissipation Factor  0.011
@Frequency 100 Hz
0.011
@Frequency 100 Hz
IEC 60250
 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
CTE, linear, Parallel to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359
Melting Point 167 °C333 °F10 K/min
 167 °C333 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FASTM Test
 140 °C284 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75
 77.0 °C171 °FASTM Test
Vicat Softening Point 130 °C266 °F(50 °C/h / 50N) - B/50; ISO 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedYes
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® N2720 M63 30% Mineral Filled POM
BASF Ultraform® H 2320 006 Q600 POM
BASF Ultraform® N 2640 Z4 BK140 Q600 POM
BASF Ultraform® N 2640 Z6 UNC POM
BASF Ultraform® N 2200 G53 UNC Q600 25% Glass Filled POM

PBASF9108 / 84872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.