MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum 2219-T31
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes: Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A92219; ISO AlCu6Mn; Aluminium 2219-T31; AA2219-T31; Al2219-T31
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.84 g/cc0.103 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 100100500 kg load with 10 mm ball
Hardness, Knoop 126126Converted from Brinell Hardness Value
Hardness, Rockwell A 41.241.2Converted from Brinell Hardness Value
Hardness, Rockwell B 6363Converted from Brinell Hardness Value
Hardness, Vickers 113113Converted from Brinell Hardness Value
Tensile Strength, Ultimate 359 MPa52000 psiAA; Typical
 >= 315 MPa
@Thickness 0.508 - 0.991 mm
>= 45700 psi
@Thickness 0.0200 - 0.0390 in
Sheet
 >= 315 MPa
@Thickness 1.02 - 6.32 mm
>= 45700 psi
@Thickness 0.0400 - 0.249 in
Sheet
 >= 290 MPa
@Diameter <=12.7 mm
>= 42100 psi
@Diameter <=0.499 in
Wire, rod, bar, and shapes (extruded)
 >= 290 MPa
@Diameter <=12.7 mm
>= 42100 psi
@Diameter <=0.499 in
Extruded tube
 >= 310 MPa
@Diameter 12.7 - 76.17 mm
>= 45000 psi
@Diameter 0.500 - 2.999 in
Wire, rod, bar, and shapes (extruded)
 >= 310 MPa
@Diameter 12.7 - 76.17 mm
>= 45000 psi
@Diameter 0.500 - 2.999 in
Extruded tube
Tensile Strength, Yield 248 MPa36000 psiAA; Typical
 >= 195 MPa
@Thickness 1.02 - 6.32 mm
>= 28300 psi
@Thickness 0.0400 - 0.249 in
Sheet
 >= 200 MPa
@Thickness 0.508 - 0.991 mm
>= 29000 psi
@Thickness 0.0200 - 0.0390 in
Sheet
 >= 180 MPa
@Diameter <=12.7 mm
>= 26100 psi
@Diameter <=0.499 in
Wire, rod, bar, and shapes (extruded)
 >= 180 MPa
@Diameter <=12.7 mm
>= 26100 psi
@Diameter <=0.499 in
Extruded tube
 >= 185 MPa
@Diameter 12.7 - 76.17 mm
>= 26800 psi
@Diameter 0.500 - 2.999 in
Wire, rod, bar, and shapes (extruded)
 >= 185 MPa
@Diameter 12.7 - 76.17 mm
>= 26800 psi
@Diameter 0.500 - 2.999 in
Extruded tube
Elongation at Break  8.0 %
@Thickness 0.508 - 0.991 mm
8.0 %
@Thickness 0.0200 - 0.0390 in
Sheet
 10 %
@Thickness 1.02 - 6.32 mm
10 %
@Thickness 0.0400 - 0.249 in
Sheet
 17 %
@Thickness 1.59 mm
17 %
@Thickness 0.0625 in
AA; Typical
 14 %
@Diameter <=12.7 mm
14 %
@Diameter <=0.499 in
Wire, rod, bar, and shapes (extruded)
 14 %
@Diameter 12.7 - 76.17 mm
14 %
@Diameter 0.500 - 2.999 in
Wire, rod, bar, and shapes (extruded)
 14 %
@Diameter <=12.7 mm
14 %
@Diameter <=0.499 in
Extruded tube
 14 %
@Diameter 12.7 - 76.17 mm
14 %
@Diameter 0.500 - 2.999 in
Extruded tube
Modulus of Elasticity 73.1 GPa10600 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Machinability 70 %70 %0-100 Scale of Aluminum Alloys
Shear Modulus 27.0 GPa3920 ksiEstimated from similar Al alloys.
Shear Strength 250 MPa36300 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000615 ohm-cm
@Temperature 20.0 °C
0.00000615 ohm-cm
@Temperature 68.0 °F
AA; Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  20.8 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.6 µin/in-°F
@Temperature -58.0 - 68.0 °F
 22.3 µm/m-°C
@Temperature 20.0 - 100 °C
12.4 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 22.5 µm/m-°C
@Temperature 20.0 - 100 °C
12.5 µin/in-°F
@Temperature 68.0 - 212 °F
 23.4 µm/m-°C
@Temperature 20.0 - 200 °C
13.0 µin/in-°F
@Temperature 68.0 - 392 °F
 24.1 µm/m-°C
@Temperature 20.0 - 300 °C
13.4 µin/in-°F
@Temperature 68.0 - 572 °F
 24.4 µm/m-°C
@Temperature 20.0 - 300 °C
13.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.864 J/g-°C0.207 BTU/lb-°F
Thermal Conductivity 112 W/m-K780 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 543 - 643 °C1010 - 1190 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting is not eliminated by homogenization.
Solidus 543 °C1010 °FAA; Typical
Liquidus 643 °C1190 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 535 °C995 °F
Aging Temperature 163 - 191 °C325 - 375 °Ffrom 18 to 36 hr at temperature
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.5 - 93.8 %91.5 - 93.8 %As remainder
Copper, Cu 5.8 - 6.8 %5.8 - 6.8 %
Iron, Fe <= 0.30 %<= 0.30 %
Magnesium, Mg <= 0.02 %<= 0.02 %
Manganese, Mn 0.20 - 0.40 %0.20 - 0.40 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.20 %<= 0.20 %
Titanium, Ti 0.02 - 0.10 %0.02 - 0.10 %
Vanadium, V 0.05 - 0.15 %0.05 - 0.15 %
Zinc, Zn <= 0.10 %<= 0.10 %
Zirconium, Zr 0.10 - 0.25 %0.10 - 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2219-O
Aluminum 2219-T351
Aluminum 2219-T87
Aluminum 2219-T6
Aluminum 2219-T37

MA2219T31 / 8927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.