MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aperam Dilver® P1 Cold Rolled Strip
Categories: Metal; Ferrous Metal

Material Notes: Dilver P1® is an iron-nickel-cobalt alloy with a CTE matched to borosilicate glass and ceramics. Typical applications are hybrid circuit casings, transistor and optoelectronic component cases and bases, electronic tubes (power, X rays), hermetic feedthroughs, SAW filters and oscillator housings.

International standards: ASTM F15 - DIN 17745 - W 1.3981 - A 54-301 - SEW 385

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.25 g/cc0.298 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 160160Annealed
 220220Hard Temper
Tensile Strength, Ultimate 540 MPa78300 psiAnnealed
 700 MPa102000 psiHard Temper
Tensile Strength, Yield 380 MPa55100 psiAnnealed
 680 MPa98600 psiHard Temper
Elongation at Break 9.0 %9.0 %Hard Temper
 30 %30 %Annealed
Tensile Modulus 139 GPa20200 ksiYoung's, Annealed
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000049 ohm-cm0.000049 ohm-cm
Curie Temperature 425 °C797 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.60 - 5.20 µm/m-°C
@Temperature 30.0 - 400 °C
2.56 - 2.89 µin/in-°F
@Temperature 86.0 - 752 °F
 5.10 - 5.50 µm/m-°C
@Temperature 30.0 - 450 °C
2.83 - 3.06 µin/in-°F
@Temperature 86.0 - 842 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity 17.5 W/m-K121 BTU-in/hr-ft²-°F
Melting Point 1450 °C2640 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 17 %17 %
Iron, Fe 54 %54 %
Nickel, Ni 29 %29 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe MP35N® Alloy
Sandvik Bioline F562/F562LTi Wire
Fused Quartz
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Carpenter Invar 36® Alloy, Cold Rolled Strip

NPERA047 / 194836

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.