MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Bioline F562/F562LTi Wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik Bioline F562 is a nonmagnetic Nickel-cobalt base alloy that has a unique combination of properties: ultra high strength, toughness, ductility and excellent corrosion resistance. Sandvik Bioline F562LTi is the low titanium version of Sandvik Bioline F562. The alloy is cold worked to obtain strength level of 17902205 MPa (260 to 320 ksi). It can also be aged in the work hardened condition to achieve higher strengths. A leading material for permanent implants, Sandvik Bioline F562 is vacuum melted in multiple steps for extreme cleanliness. Sandvik Bioline F562 is resistant to corrosion in hydrogen sulfide, salt water and other chloride solutions as well as mineral acids (nitric, hydrochloric, sulfuric). In addition, it has exceptional resistance to crevice and stress corrosion cracking having been operationally proven in sea water and hostile environments. For medical use, Sandvik delivers F562 with the highest surface finish (Medical class) in order to maximize the fatigue strength, which is critical in implant devices such as lead wires for pacemakers and heart valve supports.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.40 g/cc0.303 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9090Annealed
Hardness, Rockwell C 4343Cold worked
 5151Aged 593°C- 4 hrs
Tensile Strength, Ultimate 896 MPa130000 psiAnnealed
 1379 MPa200000 psiHot worked
 2034 MPa295000 psiAged 593°C- 4 hrs
Tensile Strength, Yield  >= 379 MPa
@Strain 0.2 %
>= 55000 psi
@Strain 0.2 %
Annealed
 >= 1310 MPa
@Strain 0.2 %
>= 190000 psi
@Strain 0.2 %
Hot worked
 >= 1965 MPa
@Strain 0.2 %
>= 285000 psi
@Strain 0.2 %
Aged 593°C- 4 hrs
Elongation at Break 2.0 %2.0 %Hot worked
 2.0 %2.0 %Aged 593°C- 4 hrs
 65 %65 %Annealed
Modulus of Elasticity 232 GPa33600 ksiAnnealed
 234 GPa33900 ksiCold worked and aged
Poissons Ratio 0.380.38Annealed; Calculated
 0.450.45Cold worked and aged; Calculated
Shear Modulus 80.9 GPa11700 ksiCold worked and aged
 83.8 GPa12200 ksiAnnealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.2 µm/m-°C
@Temperature 100 °C
6.22 µin/in-°F
@Temperature 212 °F
Thermal Conductivity 11.2 W/m-K77.7 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 20 %20 %
Cobalt, Co 35 %35 %
Molybdenum, Mo 10 %10 %
Nickel, Ni 35 %35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe MP35N® Alloy
Aperam N485 Cold Rolled Strip
Aperam N475 Cold Rolled Strip
Aperam Dilver® P1 Cold Rolled Strip
3D Systems LaserForm® Maraging Steel (B), AS BUILT

NSANDV5200 / 199764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.