MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Performance Features: Manufactures of technical parts can achieve the highest levels of:
  • Wear and tear strength
  • Dimensional stability
  • Oil resistance
  • Low compression set
  • Dynamic load performance
  • Elasticity and flexibility
  • Temperature performance
  • Processing consistency

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Linear Mold Shrinkage 0.030 cm/cm0.030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ASTM D2240
Hardness, Shore D 1818ASTM D2240
Tensile Strength at Break 25.5 MPa3700 psiASTM D412
Elongation at Break 900 %900 %ASTM D412
100% Modulus 3.52 MPa
@Strain 100 %
510 psi
@Strain 100 %
ASTM D412
300% Modulus 5.52 MPa
@Strain 300 %
800 psi
@Strain 300 %
ASTM D412
Rebound 54 %54 %Bayshore; ASTM D2632
Tear Strength 63.1 kN/m360 pliASTM D624
Abrasion 5555mm3; ISO 34-1
Compression Set  43 %
@Temperature 22.8 °C,
Time 252000 sec
43 %
@Temperature 73.0 °F,
Time 70.0 hour
ASTM D395
 54 %
@Temperature 70.0 °C,
Time 86400 sec
54 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 - 170 °C284 - 338 °FTMA Melt Range

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU)
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade

PHUQ120 / 159493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.