MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® A-401C with 60 MT Black Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Fully precompounded for O-ring curative level
  • Improved compression molding with increased mold flow, easier mold release, and less mold fouling
  • Improved extrusion
  • Increased cure rate
  • Improved compression set resistance
  • Same mold shrinkage as Viton® E-60C

Applications

  • Viton® A-401C is highly recommended for O-rings, extruded cord, gaskets, seals, and profiles. Viton® A-401C can be formulated to meet fluoroelastomer specifications Mil-R-83248B, AMS 7276D, and AMS 7259A.

    Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Mooney Viscosity 115
    @Temperature 121 °C
    115
    @Temperature 250 °F
    ML (1+10), Uncompounded Viton; ASTM D1646
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 8787No Postcure; ASTM D2240
     909024 hours Postcure; ASTM D2240
    Tensile Strength at Break 9.20 MPa1330 psiNo Postcure; ASTM D412
     14.5 MPa2100 psi24 hours Postcure; ASTM D412
    Elongation at Break 130 %130 %24 hours Postcure; ASTM D412
     180 %180 %No Postcure; ASTM D412
    100% Modulus  7.10 MPa
    @Strain 100 %
    1030 psi
    @Strain 100 %
    No Postcure; ASTM D412
     11.9 MPa
    @Strain 100 %
    1730 psi
    @Strain 100 %
    24 hours Postcure; ASTM D412
    Compression Set  15 %
    @Temperature 23.0 °C,
    Time 252000 sec
    15 %
    @Temperature 73.4 °F,
    Time 70.0 hour
    O-Rings; ASTM D395B
     21 %
    @Temperature 200 °C,
    Time 252000 sec
    21 %
    @Temperature 392 °F,
    Time 70.0 hour
    O-Rings; ASTM D395B
     29 %
    @Temperature 200 °C,
    Time 605000 sec
    29 %
    @Temperature 392 °F,
    Time 168 hour
    O-Rings; ASTM D395B
     38 %
    @Temperature 200 °C,
    Time 1.21e+6 sec
    38 %
    @Temperature 392 °F,
    Time 336 hour
    O-Rings; ASTM D395B
     46 %
    @Temperature 232 °C,
    Time 252000 sec
    46 %
    @Temperature 450 °F,
    Time 70.0 hour
    O-Rings; ASTM D395B
     
    Processing PropertiesMetricEnglishComments
    Processing Temperature  177 °C
    @Time 601 sec
    351 °F
    @Time 0.167 hour
    Slab Cure
     232 °C
    @Time 86400 sec
    450 °F
    @Time 24.0 hour
    Postcure
     
    Descriptive Properties
    Formulation as Tested100A401C
     3MgO
     6Ca(OH)2
     60MT Black

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    AlphaGary PVC 2235RSM-100 CLEAR 000X Polyvinyl Chloride Thermoplastic
    Chemours Viton® AHV
    Precision Polymer Engineering E90Q Ethylene Propylene Rubber
    AlphaGary PVC 2212-100 CLEAR 0003 Polyvinyl Chloride Thermoplastic
    Chemours Viton® A-700 with 65 phr N990 Carbon Black

    PDVC9914 / 170555

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.