MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AlphaGary PVC 2235RSM-100 CLEAR 000X Polyvinyl Chloride Thermoplastic
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded; PVC, Transparent

Material Notes: Extraction and lipid resistant, non-migrating for use in contact with polystyrene, polycarbonate, etc. Good melt flow, low processing temperatures, superior heat stability & good mold release for connectors, accessories to IV bags, catheters, etc.
Formulated for injection molding or extrusion

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 100 - 110100 - 110
Hardness, Shore D 6161
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Clear; thickness not specified
 
Descriptive Properties
DEHP FreeYes
Phthalate FreeYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ SM 1300 Polyolefin Plastomer
Precision Polymer Engineering E90Q Ethylene Propylene Rubber
Seals Eastern 7204 Ethylene-Propylene Rubber
Chemours Viton® A-700 with 65 phr N990 Carbon Black
Chemours Viton® A-401C with 60 MT Black Fluoroelastomer Compound

PGARY9957 / 140743

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.