MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® XL07407 Copolymer
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes:

Applications
PETROTHENE XL 07407 is especially formulated for use in flame retardant, primary insulation for low voltage automotive wire and cable applications (SAE J1128), and for UL applications including 125°C appliance wire and SIS. XL 7407 is a non-tarnishing, non-halogenated, flame retardant, chemically crosslinkable compound. Non-discoloring antioxidant and special active peroxide have been added to ensure thermal stability during processing and optimum curing results.

Processing Techniques
XL 07407, like other crosslinkable polyolefin compounds, can be extruded as wire and cable insulation by means of a conventional extruder with a continuous vulcanization tube. Below are suggested extrusion conditions for XL 07407. These conditions are intended as general guidelines only and are not optimum values, since manufacturing variables such as extruder type and size, continuous vulcanization tube design and cable construction all have an effect on processing of crosslinkable compounds.

Additional Suggestions
Maximum screen pack of 40 mesh
Little or no die land
No predrying normally required
Compression ratio of 2:1-3:1
"Mixing" screw can be used if properly designed to prevent excessive heat build-up
Dies should be cleaned frequently to reduce compound build-up
Approximately 20% oversize dies are recommended
The die area should be cooled up to 20°F by hot water or oil to reduce die build-up
Conductors should be cleaned or flame treated to remove any trace drawing oils prior to extrusion
Chemical or taped separators may be necessary to provide peelable adhesion over certain conductor types
Curing line steam temperature should be at least 400°F (205°C)
Residence time in the steam should be at least 25 seconds

Physical Properties
All properties determined from compression molded, press cured plaques. The values listed for physical and electrical properties are nominal values only and are subject to normal variations consistent with the test methods and/or variations found acceptable to the industry.

This product is from the former Equistar product line.

Key Words: Automotive SAE J1128; Appliance Wire 125°C; Non-halogenated; Non-tarnishing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.7 MPa3000 psi101% retention after aging 7 days at 165°C.; ASTM D638
Elongation at Break 220 %220 %98% retention after aging 7 days at 165°C.; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 26 %26 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Feed Temperature 107 - 113 °C225 - 235 °F
Zone 2 107 - 113 °C225 - 235 °F
Zone 3 116 - 127 °C240 - 260 °FZone 3-X
Adapter Temperature 116 - 238 °C240 - 460 °F
Die Temperature 116 - 127 °C240 - 260 °F
Melt Temperature 116 - 127 °C240 - 260 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® XL07414 Copolymer
LyondellBasell Petrothene® XL07425 Copolymer
LyondellBasell Hifax TRC 779X SHS BLACK Thermoplastic Olefinic Elastomer, mineral Filled
LyondellBasell Petrothene® YR19548 Polyolefin Compound
UCAR Carbon UCAR® CBY Extruded Graphite

PEQU0304 / 36738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.