MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

UCAR Carbon UCAR® CBY Extruded Graphite
Categories: Carbon; Graphite

Material Notes: Grade CBY is a general purpose, cost effective extruded graphite with improved strength, structure and density characteristics. It is a low ash graphite for superior oxidation resistance.

Typical Applications:

  • Heat treating boats and trays
  • Furnace parts
  • Fused refractory molds
  • Aluminum runout tables
  • Induction furnace susceptors
  • Refractory Systems applications such as blast furnace and submerged arc furnace linings

Tabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³
Particle Size <= 750 µm<= 750 µm
Ash 0.090 %0.090 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 16.5 MPa2400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000840 ohm-cm0.000840 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.50 µm/m-°C
@Temperature 20.0 - 100 °C
1.39 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 150 W/m-K1040 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poco Graphite ZXF-5Q Industrial Grade Graphite
UCAR Carbon UCAR® PGX Pressure Molded Graphite
Poco Graphite ACF-10Q Industrial Grade Graphite
Poco Graphite AXF-5Q Industrial Grade Graphite
UCAR Carbon UCAR® ATA Isostatic Molded Graphite

CGRAFT00 / 1166

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.