MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

UCAR Carbon UCAR® PGX Pressure Molded Graphite
Categories: Carbon; Graphite

Material Notes: Available in low ash monolithic sizes as large as 73" diameter, Grade PGX has excellent erosion resistance and thermal properties.

Typical Applications:

  • Fluidized bed reactors
  • Centrifugal casting molds
  • Large diameter molds and crucibles
  • Monolithic composite tooling parts
  • Induction and vacuum furnace parts
  • Heat exchangers
  • Chemical process equipment

Tabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.73 g/cc0.0625 lb/in³
Particle Size <= 750 µm<= 750 µm
Ash 0.070 %0.070 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 11.0 MPa1600 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00101 ohm-cm0.00101 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.20 µm/m-°C
@Temperature 20.0 - 100 °C
1.22 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 125 W/m-K868 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UCAR Carbon UCAR® ATA Isostatic Molded Graphite
UCAR Carbon UCAR® PGW Pressure Molded Graphite
Poco Graphite ACF-10Q Industrial Grade Graphite
Poco Graphite ZXF-5Q Industrial Grade Graphite
UCAR Carbon UCAR® ATR Isostatic Molded Graphite

CGRAFT07 / 1173

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.