MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Poco Graphite ZXF-5Q Industrial Grade Graphite
Categories: Carbon; Graphite

Material Notes: SSH hardness is 86.

General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small particle size allow fabrication of complex components containing tight tolerances. Post synthesis treatments available include purification or impregnation with resins, oxidation inhibitors, or metals. Surface treatments offer improved wear characteristics and particle reduction.

Some applications of Poco specialty graphites include anode plates for wet cells, fuel cell plates for solid polymer cells, air bearings, hot gas valves, high temperature bearings, bushings, and seals, hot press dies and rams, furnace furniture/fixturing, rocket engine nozzles, molten metal casting components, vacuum furnace heating elements, space vehicle nose cones, mirrors and optical structures, and satellite heat shields.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.78 g/cc0.0643 lb/in³
Open Porosity 80 %80 %
Porosity 20 %20 %
Particle Size 1.0 µm1.0 µm
Pore Size 0.300 microns0.0118 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Tensile Strength, Yield 79.0 MPa11500 psi
Elongation at Yield 0.78 %0.78 %
Modulus of Elasticity 14.5 GPa2100 ksi
Flexural Strength 112 MPa16200 psi
Compressive Strength 175 MPa25400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00195 ohm-cm0.00195 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.10 µm/m-°C4.50 µin/in-°F
Thermal Conductivity 70.0 W/m-K486 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poco Graphite ACF-10Q Industrial Grade Graphite
Poco Graphite AXF-5Q Industrial Grade Graphite
UCAR Carbon UCAR® CBY Extruded Graphite
UCAR Carbon UCAR® PGW Pressure Molded Graphite
UCAR Carbon UCAR® PGX Pressure Molded Graphite

CPOCO08 / 85585

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.