MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 9659DU Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; with special UV stabilizers; transparent up to 6 mm wall thickness; very good hydrolysis and microbial resistance; Application; Ski boot shells; Hoses, non-reinforced

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9797ISO 868
Hardness, Shore D 5858ISO 868
Tensile Strength, Ultimate 52.7 MPa7640 psi200 mm/min; DIN 53504
Tensile Stress at Strain  10.9 MPa
@Strain 10 %
1580 psi
@Strain 10 %
200 mm/min; DIN 53504
 19.6 MPa
@Strain 50 %
2840 psi
@Strain 50 %
200 mm/min; DIN 53504
 25.4 MPa
@Strain 100 %
3680 psi
@Strain 100 %
200 mm/min; DIN 53504
 31.2 MPa
@Strain 300 %
4530 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 324 %324 %200 mm/min; DIN 53504
Tensile Modulus  0.128 GPa
@Temperature 60.0 °C
18.6 ksi
@Temperature 140 °F
storage; ISO 6421-1,-4
 0.502 GPa
@Temperature 20.0 °C
72.8 ksi
@Temperature 68.0 °F
storage; ISO 6421-1,-4
 2.00 GPa
@Temperature -20.0 °C
290 ksi
@Temperature -4.00 °F
storage; ISO 6421-1,-4
Flexural Modulus 0.165 GPa23.9 ksi2 mm/min; ISO 178
Rebound 29 %29 %Resilience; ISO 4662
Tear Strength 89.0 kN/m508 pli500 mm/min; ISO 34-1
Abrasion 2020mm³, Method A; ISO 4649
Compression Set  37 %
@Temperature 23.0 °C
37 %
@Temperature 73.4 °F
72 hr; ISO 815
 82 %
@Temperature 70.0 °C
82 %
@Temperature 158 °F
24 hr; ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 - 235 °C401 - 455 °FExtrusion
 220 - 240 °C428 - 464 °FInjection
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection
Drying Temperature 110 °C230 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 9650DU Polyurethane
Covestro Desmopan® 9873DU Polyurethane
Covestro Desmopan® 9395AU Polyurethane
Covestro Desmopan® 9662DU Polyurethane
Covestro Desmopan® 9665DU Polyurethane

PB09820 / 92660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.