MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 9665DU Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; with special UV stabilizers; transparent up to 6 mm wall thickness; very good hydrolysis and microbial resistance; Application; Ski boot shells; Hoses, non-reinforced; Pneumatic hoses

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9898ISO 868
Hardness, Shore D 6565ISO 868
Tensile Strength, Ultimate 53.4 MPa7750 psi200 mm/min; DIN 53504
Tensile Stress at Strain  15.8 MPa
@Strain 10 %
2290 psi
@Strain 10 %
200 mm/min; DIN 53504
 23.6 MPa
@Strain 50 %
3420 psi
@Strain 50 %
200 mm/min; DIN 53504
 28.4 MPa
@Strain 100 %
4120 psi
@Strain 100 %
200 mm/min; DIN 53504
 37.8 MPa
@Strain 300 %
5480 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 349 %349 %200 mm/min; DIN 53504
Tensile Modulus  0.215 GPa
@Temperature 60.0 °C
31.2 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.816 GPa
@Temperature 20.0 °C
118 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 2.25 GPa
@Temperature -20.0 °C
326 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
Flexural Modulus 0.270 GPa39.2 ksi2 mm/min; ISO 178
Rebound 40 %40 %Resilience; ISO 4662
Tear Strength 208 kN/m1190 pli500 mm/min; ISO 34-1
Abrasion 1919mm³, Method A; ISO 4649
Compression Set  39 %
@Temperature 23.0 °C
39 %
@Temperature 73.4 °F
72 hr; ISO 815
 50 %
@Temperature 70.0 °C
50 %
@Temperature 158 °F
24 hr; ISO 815
 28 %
@Temperature 70.0 °C,
Time 86400 sec
28 %
@Temperature 158 °F,
Time 24.0 hour
Method C; ISO 815-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 - 235 °C401 - 455 °FExtrusion
 220 - 235 °C428 - 455 °FInjection
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection
Drying Temperature 110 °C230 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 9873DU Polyurethane
Covestro Desmopan® 9659DU Polyurethane
Covestro Desmopan® 3072D Polyurethane
Covestro Desmopan® 3660DU Polyurethane
Covestro Desmopan® 85786A Polyurethane

PB09822 / 92662

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.