MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik DC03 Cemented Carbide for Woodworking  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: Sandvik DC03 grade has been developed to give superior tool life in demanding applications. This extra fine grain size grade with low binder phase content offers a superior hardness and corrosion/oxidation resistance. The extra fine microstructure of DC03 gives the opportunity to reach superior cutting edge quality.

Features:

  • Extra fine grain size
  • Superior abrasion resistance
  • Superior cutting edge quality
  • Superior corrosion and oxidation resistance
  • Binderphase content 3%
  • Codes: ISO K01, US C4

    Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 15.25 g/cc0.5509 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell A 9494
    Hardness, Vickers 1900190030
    Flexural Strength 2100 MPa305000 psiTransverse Rupture; ISO 3327

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    SSAB Tunnplat Docol® DC01 (Fe P01) Deep-drawing Steel
    SSAB Tunnplat Docol® DC04 (Fe P04) Deep-drawing Steel
    Aluminum 6082-T6
    ArcelorMittal 53 High formability steel for drawing, Cold rolled
    Sandvik HF10 Extra-Fine Cemented Carbide for Metal Forming Applications

    NSANDV041 / 18935

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.