MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Samyang Trirex® PC-3025N2 10 MFI Flame Retardant Clear Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Polymer Technology & Services, LLC (PTS)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %24 hours at 73°F
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 63.5 MPa
@Thickness 3.17 mm
9210 psi
@Thickness 0.125 in
Elongation at Break 100 %
@Thickness 3.17 mm
100 %
@Thickness 0.125 in
Flexural Yield Strength 84.0 MPa
@Thickness 3.17 mm
12200 psi
@Thickness 0.125 in
Flexural Modulus 3.10 GPa
@Thickness 3.17 mm
450 ksi
@Thickness 0.125 in
Izod Impact, Notched 5.87 J/cm
@Thickness 3.17 mm
11.0 ft-lb/in
@Thickness 0.125 in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+16 ohm-cm4.00e+16 ohm-cmASTM D257
Dielectric Constant 2.82.8ASTM D150
Dielectric Strength 30.0 kV/mm
@Thickness 3.00 mm
762 kV/in
@Thickness 0.118 in
ASTM D149
Dissipation Factor 0.00820.0082ASTM D150
Arc Resistance 120 sec
@Thickness 3.00 mm
120 sec
@Thickness 0.118 in
High Voltage, Low Current; ASTM D495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 86 %
@Thickness 3.00 mm
>= 86 %
@Thickness 0.118 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 266 - 282 °C510 - 540 °F
Middle Barrel Temperature 271 - 288 °C520 - 550 °F
Front Barrel Temperature 282 - 304 °C540 - 580 °F
Nozzle Temperature 277 - 310 °C530 - 590 °F
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 71.1 - 110 °C160 - 230 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 4 hour3 - 4 hour
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi
Back Pressure 0.345 - 1.38 MPa50.0 - 200 psi
Clamp Pressure 27.6 - 68.9 MPa4000 - 10000 psi
Cycle Time - Injection 1.0 - 2.5 sec1.0 - 2.5 sec
Cycle Time - Cooling 5.0 - 40 sec5.0 - 40 sec
Vent Depth 0.00200 - 0.00800 cm0.000787 - 0.00315 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
Injection Speed- Edge GateSlow-Medium
Injection Speed- Tab GateMedium-Fast
Injection Speed- Tunnel GateFast
Shot Size40-60%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2608 Polycarbonate
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
Covestro Makrolon® 1837 MAS081 Polycarbonate
Samyang Trirex® 3025N1 Polycarbonate, Flame Retardant
Overview of materials for Polycarbonate, 20% Glass Filled

PLBS18 / 50472

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.