MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NYCOA 2256 30% Glass Filled Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: 30% glass filled, impact modified nylon 6

Information provided by NYCOA, Inc.

Key Words: PA 6, Polyamide 6, Nylon 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183-A
Water Absorption 0.95 %0.95 %ISO METHOD 62
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 131 MPa19000 psiISO METHOD 527
Elongation at Break 8.0 %8.0 %ISO METHOD 527
Flexural Yield Strength 160 MPa23200 psiISO METHOD 176
Flexural Modulus 6.813 GPa988.2 ksiISO METHOD 178
Izod Impact, Notched 1.18 J/cm2.21 ft-lb/inISO METHOD 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 °C430 °FISO METHOD 3146C
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 °C482 °F
Rear Barrel Temperature 225 °C437 °F
Middle Barrel Temperature 230 °C446 °F
Front Barrel Temperature 250 °C482 °F
Nozzle Temperature 250 °C482 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 76.0 °C169 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
Domo Technyl® C216V30 30% Glass Filled Nylon 6
NYCOA 2037 15% Glass Filled Nylon 6
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, 30% Glass Fiber Filled

PNYCOA22 / 55568

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.