MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Pro-fax PD702NW Polypropylene Homopolymer, Nucleated/Antistat
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Primary Processing Method: Injection Molding

Key Features: nucleated and antistatic, high flow polypropylene homopolymer resin, FDA acceptable, short cycle time for high productivity, resists dust pickup, enhanced stiffness, good flow properties

Applications: large articles, thin wall parts

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: Pro-fax PD702N nucleated, antistatic, high flow, controlled rheology polypropylene homopolymer resin is designed for injection molding. It is available in pellet form. It meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792B
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9393ASTM D785A
Tensile Strength, Yield 34.0 MPa4930 psiASTM D638
Elongation at Yield 11 %11 %ASTM D638
Flexural Modulus, 1% Secant 1300 MPa189000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 0.370 J/cm0.693 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C232 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer
Braskem C758-80NA Polypropylene Impact Copolymer
LyondellBasell Pro-fax™ SR257M Polypropylene Copolymer
Total PPC 4720 WZ Polypropylene, Impact Copolymer

PMO087 / 53518

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.