MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tipco Tipcofil® KMX 800 FR - UL94-V0 Flame Retardant, Highly Filled PBT/PC Alloy, with High Heat Stability
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Highly Filled, Flame Retardant PBT/PC Alloy, for Injection Molding of "Ceramic Effect" Parts

Applications: Electrical & Appliances

Processing: Injection Molding

Information provided by the Manufacturer, Tipco Industries Ltd., India.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955
Melt Flow 45 g/10 min45 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiASTM D638
Elongation at Break >= 5.0 %>= 5.0 %ASTM D638
Flexural Yield Strength 100 MPa14500 psiASTM D790
Flexural Modulus 4.70 GPa682 ksiASTM D790
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ASTM D256
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FASTM D648
Vicat Softening Point 200 °C392 °FASTM D1525
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 °C518 °F
Rear Barrel Temperature 250 °C482 °F
Middle Barrel Temperature 260 °C500 °F
Front Barrel Temperature 275 °C527 °F
Nozzle Temperature 265 °C509 °F
Mold Temperature 105 °C221 °F
Drying Temperature 90.0 °C194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems Accura® Xtreme Plastic for SLA® Systems
Mearthane Durethane™ F DF-235A Closed Cell Foam Polyurethane
MRC Polymers NAXALOY™ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled
Momentive Performance Materials RTV1473 Black Adhesive Sealant, FIPG
Mitsubishi Iupilon® MB 2105 PC/Polyester

PTIP690 / 70335

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.