MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MRC Polymers NAXALOY™ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Good chemical resistance, impact and heat resistance
  • Available in Black Only
  • Can be UV Stabilized
  • Internal and external lubricant can be added.

Information provided by MRC Polymers Inc.

Key Words: PC, PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 250 °C
18 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 77.98 MPa11310 psiISO 527
Flexural Strength 116.97 MPa16965 psiISO 178
Flexural Modulus 3.7490 GPa543.75 ksiISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C226 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 270 °C464 - 518 °F
Middle Barrel Temperature 245 - 275 °C473 - 527 °F
Front Barrel Temperature 250 - 280 °C482 - 536 °F
Nozzle Temperature 245 - 275 °C473 - 527 °F
Melt Temperature 255 - 275 °C491 - 527 °F
Mold Temperature 62.8 - 92.8 °C145 - 199 °F
Drying Temperature 107 - 113 °C225 - 235 °F
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content <= 0.020 %<= 0.020 %
Dew Point <= -17.8 °C<= 0.000 °F
Drying Air Flow Rate 22.7 - 28.3 l/min0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 34.5 - 172 MPa5000 - 25000 psi
Back Pressure 0.000 - 0.517 MPa0.000 - 75.0 psi
Shot Size 50 - 80 %50 - 80 %
Vent Depth 0.00127 - 0.00203 cm0.000500 - 0.000800 in
Cushion 0.635 cm0.250 in
Screw Speed 50 - 80 rpm50 - 80 rpm
 
Descriptive Properties
Fill RateModerate to Fast
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupox® TE5000GU PBT+PC
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled
MRC Polymers NAXALOY™ 794A1 Polycarbonate & Polyester Blend
MRC Polymers NAXALOY™ 795 Polycarbonate & Polyester Blend

PMRC022 / 89451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.