MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MRC Polymers NAXALOY™ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Good chemical resistance, impact and heat resistance
  • Available in Black Only
  • Can be UV Stabilized
  • Internal and external lubricant can be added.

Information provided by MRC Polymers Inc.

Key Words: PC, PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 in/inASTM D955
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 11310 psiISO 527
Flexural Strength 16.965 ksiISO 178
Flexural Modulus 543.75 ksiISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 226 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 464 - 518 °F
Middle Barrel Temperature 473 - 527 °F
Front Barrel Temperature 482 - 536 °F
Nozzle Temperature 473 - 527 °F
Melt Temperature 491 - 527 °F
Mold Temperature 145 - 199 °F
Drying Temperature 225 - 235 °F
Dry Time 3 - 4 hour
Moisture Content <= 0.020 %
Dew Point <= 0.000 °F
Drying Air Flow Rate 0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 5000 - 25000 psi
Back Pressure 0.000 - 75.0 psi
Shot Size 50 - 80 %
Vent Depth 0.000500 - 0.000800 in
Cushion 0.250 in
Screw Speed 50 - 80 rpm
 
Descriptive Properties
Fill RateModerate to Fast
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Lupox® TE5000GU PBT+PC
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled
MRC Polymers NAXALOY™ 794A1 Polycarbonate & Polyester Blend
MRC Polymers NAXALOY™ 795 Polycarbonate & Polyester Blend

PMRC022 / 89451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.