MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TriStar Ultracomp UC-500 Composite Bearing
Categories: Polymer; Thermoplastic

Material Notes: Ultracomp UC-500 - Multiple sources of lubrication make this Ultracomp an excellent choice for full rotary or higher speed linear applications. High strength, high impact resistance and long wear life.

This family of composite materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of cryogenic to over 360°F with and without additional lubricants.

Ultracomp Bearing Grade Composite: Laminates composed of synthetic fabrics impregnated by thermosetting resins and solid lubricant fillers. Material is available in tubes and sheets. Ideally suited for non-lubricated ultra high-load/low-speed applications that require a low coefficient of friction. Operates well in demanding and destructive environments. Suitable for use in steam, wet, dry, or vacuum environments. Rc 35 or higher steel mating surface. Markets for Ultracomp Bearing Grade Composite include Agricultural, Appliances, Automotive, Construction, Industrial, and Transportation.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/cc
Water Absorption <= 0.10 %<= 0.10 %24 hrs
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 65.5 MPa9500 psi
Flexural Strength 93.1 MPa13500 psi
Compressive Yield Strength 128 MPa18500 psiPerpendicular to Laminate
Ultimate Compressive Strength 345 MPa50000 psiPerpendicular to Laminate
Compressive Modulus 5.17 GPa750 ksiPerpendicular to Laminate
Izod Impact, Notched <= 10.7 J/cm<= 20.0 ft-lb/in
Coefficient of Friction, Static 0.150.15Dry vs. Steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 168 °C335 °FContinuous
 182 °C360 °FShort Term
Minimum Service Temperature, Air -240 °C-400 °FEmbrittlement Temp

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TriStar Ultracomp UC-400 Composite Bearing
TriStar Ultracomp UC-200 Composite Bearing
TriStar Ultracomp UC-300 Composite Bearing
TriStar TriSteel AC Metal Backed PTFE Bearing System
TriStar FCJ Composite Bearing

PTRIST985 / 99336

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.