MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kingfa JH820 Modified PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes:
    Features:
  • Excellent balance properties
  • Super high impact strength
  • High stiffness
  • Good size stability
  • Good surface, high gloss
  • High transparency

    Applications:
  • Injection molding
  • Household appliance
  • Business machine cabinet
  • Transparent plate
  • Packaging

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc
@Temperature 23.0 °C
1.20 g/cc
@Temperature 73.4 °F
ASTM D792
Water Absorption 0.12 %
@Temperature 23.0 °C,
Time 86400 sec
0.12 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Temperature 23.0 °C
0.0050 - 0.0070 in/in
@Temperature 73.4 °F
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 62.0 MPa8990 psi50mm/min; ASTM D638
Elongation at Break 100 %100 %50mm/min; ASTM D638
Flexural Strength 85.0 MPa12300 psi2mm/min; ASTM D790
Flexural Modulus 2.30 GPa334 ksi2mm/min; ASTM D790
Izod Impact, Notched 7.00 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
13.1 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohm1.00e+15 ohmASTM D257
Dielectric Strength 28.0 kV/mm711 kV/in1.6mm; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
@Thickness 6.40 mm
275 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
@Thickness 6.40 mm
266 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 300 °C<= 572 °F
Rear Barrel Temperature 240 - 270 °C464 - 518 °FStart Point: 260°C
Middle Barrel Temperature 260 - 280 °C500 - 536 °FStart Point: 265°C
Front Barrel Temperature 270 - 290 °C518 - 554 °FStart Point: 275°C
Melt Temperature 250 - 280 °C482 - 536 °FStart Point: 260°C
Mold Temperature 60.0 - 80.0 °C140 - 176 °FStart Point: 70°C
Drying Temperature 120 °C
@Time 14400 - 21600 sec
248 °F
@Time 4.00 - 6.00 hour
Pre-dry
Back Pressure 0.700 - 1.00 MPa102 - 145 psi
 
Descriptive Properties
Injection Speed60-90%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kingfa JH830 Flame Retardant PC
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Covestro Apec® RW1697 Polycarbonate
Kingfa JH830T Flame Retardant PC

PKINGF049 / 104308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.