MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC 120W Linear Low Density Polyethylene for Blown Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and optical properties.
Formulation: 1500 ppm Slip & 3000 ppm Antiblock

Typical Applications: Ice & frozen food bags, liners, produce bags, bread bags, textile & garment packaging, etc.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³load density; ASTM D1505
Thickness 30.0 microns1.18 mil
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.0 MPa1450 psiASTM D882
Film Tensile Strength at Yield, TD 9.00 MPa1310 psiASTM D882
Film Elongation at Break, MD 650 %650 %ASTM D882
Film Elongation at Break, TD 810 %810 %ASTM D882
Elmendorf Tear Strength MD 160 g160 gASTM D1922
Elmendorf Tear Strength TD 350 g350 gASTM D1922
Elmendorf Tear Strength, MD 5.33 g/micron135 g/milASTM D1922
Elmendorf Tear Strength, TD 11.67 g/micron296.4 g/milASTM D1922
Dart Drop Total Energy 600 J/cm1.12 ft-lb/milPuncture Resistance; SABIC Method
Dart Drop 4.00 g/micron102 g/milASTM D1709
Dart Drop Test 120 g0.265 lbASTM D1709
Film Tensile Strength at Break, MD 38.0 MPa5510 psiASTM D882
Film Tensile Strength at Break, TD 30.0 MPa4350 psiASTM D882
1% Secant Modulus, MD 260 MPa37700 psiASTM D882
1% Secant Modulus, TD 270 MPa39200 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100 °C212 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D1003
Gloss 90 %90 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 215 °C383 - 419 °F
Blow-up Ratio (BUR) 2.0 - 3.02.0 - 3.0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® C40 01 PA66/6 (Dry)
SABIC 6821N Linear Low Density Polyethylene for Blown Film
BASF Ultramid® C40LX 01 PA66/6 (Dry)
BASF Ultramid® B40LN 01 PA6 (Dry)
NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin

PSABICZ827 / 133023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.