MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel

Material Notes: Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W and V, gives an extremely high compressive strength, 69 HRC, combined with a very good abrasive wear resistance. For cutting tool applications Uddeholm Vanadis 60 offers a unique combination of high wear resistance, hot hardness and good toughness compared to all other HSS. The P/M process ensures a good machinability and grindability together with a good dimensional stability during heat treatment.

Vanadis 60 is characterized by:

  • High wear resistance
  • Maximum compressive strength
  • Good through hardening properties
  • Good toughness
  • Good dimensional stability on heat treatment
  • Very good temper resistance
Applications: Uddeholm Vanadis 60 is a high alloyed high performance PM high speed steel with an addition of cobalt. Uddeholm Vanadis 60 is particularly suitable for cold work tooling where highest wear resistance and highest compressive strength are required at the same time.

Key Words: W.-Nr. 1.3241
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.92 g/cc0.286 lb/in³soft annealed
 7.78 g/cc
@Temperature 600.0 °C
0.281 lb/in³
@Temperature 1112 °F
soft annealed
 7.83 g/cc
@Temperature 399 °C
0.283 lb/in³
@Temperature 750 °F
soft annealed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 340<= 340Soft annealed
Hardness, Rockwell C 62 - 6962 - 69austenitizing 1760-2156°F, temper 3 x 1hr at 1040°F
Modulus of Elasticity 248 GPa36000 ksi(hardened and tempered)
 138 GPa
@Temperature 600.0 °C
20000 ksi
@Temperature 1112 °F
hardened and tempered
 221 GPa
@Temperature 399 °C
32000 ksi
@Temperature 750 °F
hardened and tempered
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.6 µm/m-°C
@Temperature 399 °C
5.90 µin/in-°F
@Temperature 750 °F
hardened and tempered
 11.0 µm/m-°C
@Temperature 600.0 °C
6.10 µin/in-°F
@Temperature 1112 °F
hardened and tempered
Specific Heat Capacity  0.418 J/g-°C
@Temperature 20.0 °C
0.100 BTU/lb-°F
@Temperature 68.0 °F
hardened and tempered
 0.502 J/g-°C
@Temperature 399 °C
0.120 BTU/lb-°F
@Temperature 750 °F
hardened and tempered
 0.586 J/g-°C
@Temperature 600.0 °C
0.140 BTU/lb-°F
@Temperature 1112 °F
hardened and tempered
Thermal Conductivity  21.0 W/m-K
@Temperature 20.0 °C
146 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
hardened and tempered
 24.0 W/m-K
@Temperature 600.0 °C
167 BTU-in/hr-ft²-°F
@Temperature 1112 °F
hardened and tempered
 25.0 W/m-K
@Temperature 399 °C
174 BTU-in/hr-ft²-°F
@Temperature 750 °F
hardened and tempered
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.3 %2.3 %
Chromium, Cr 4.2 %4.2 %
Cobalt, Co 10.5 %10.5 %
Iron, Fe 63 %63 %As Balance
Molybdenum, Mo 7.0 %7.0 %
Tungsten, W 6.5 %6.5 %
Vanadium, V 6.5 %6.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
316 Stainless Steel, annealed sheet
304 Stainless Steel
AISI 4340 Steel, annealed, 25 mm round

NBUCOR17 / 15486

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.