MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether + Styrene-Butadiene Blend

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 - 1.10 g/cc0.0383 - 0.0397 lb/in³Average value: 1.07 g/cc Grade Count:9
Water Absorption 0.300 - 0.400 %0.300 - 0.400 %Average value: 0.356 % Grade Count:9
Moisture Absorption at Equilibrium 0.100 - 0.150 %0.100 - 0.150 %Average value: 0.128 % Grade Count:9
Linear Mold Shrinkage 0.00600 cm/cm0.00600 in/inAverage value: 0.00600 cm/cm Grade Count:9
Melt Flow 8.00 - 130 g/10 min8.00 - 130 g/10 minAverage value: 64.2 g/10 min Grade Count:9
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 - 80.0 MPa7250 - 11600 psiAverage value: 62.7 MPa Grade Count:9
Elongation at Break 20.0 - 50.0 %20.0 - 50.0 %Average value: 35.0 % Grade Count:9
Elongation at Yield 4.00 - 6.00 %4.00 - 6.00 %Average value: 5.00 % Grade Count:9
Modulus of Elasticity 2.20 - 2.80 GPa319 - 406 ksiAverage value: 2.54 GPa Grade Count:9
Charpy Impact Unnotched 5.00 J/cm² - NB23.8 ft-lb/in² - NBAverage value: 5.00 J/cm² Grade Count:9
 1.00 J/cm² - NB
@Temperature -30.0 - -30.0 °C
4.76 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 2.19 J/cm² Grade Count:9
Charpy Impact, Notched 1.60 - 3.20 J/cm²7.61 - 15.2 ft-lb/in²Average value: 2.22 J/cm² Grade Count:9
 1.60 - 3.20 J/cm²
@Temperature -30.0 - -30.0 °C
7.61 - 15.2 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.22 J/cm² Grade Count:9
Tensile Creep Modulus, 1000 hours 1850 - 1950 MPa268000 - 283000 psiAverage value: 1900 MPa Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmAverage value: 1.00e+15 ohm-cm Grade Count:9
Surface Resistance 1.00e+14 ohm1.00e+14 ohmAverage value: 1.00e+14 ohm Grade Count:9
Dielectric Constant 2.50 - 2.902.50 - 2.90Average value: 2.69 Grade Count:9
Dielectric Strength 90.0 - 95.0 kV/mm2290 - 2410 kV/inAverage value: 91.7 kV/mm Grade Count:9
Dissipation Factor 0.000500 - 0.006000.000500 - 0.00600Average value: 0.00272 Grade Count:9
Comparative Tracking Index 250 - 300 V250 - 300 VAverage value: 283 V Grade Count:9
 
Thermal PropertiesMetricEnglishComments
CTE, linear 65.0 µm/m-°C36.1 µin/in-°FAverage value: 65.0 µm/m-°C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 107 - 157 °C225 - 315 °FAverage value: 126 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 100 - 140 °C212 - 284 °FAverage value: 114 °C Grade Count:9
Vicat Softening Point 108 - 160 °C226 - 320 °FAverage value: 128 °C Grade Count:9
Flammability, UL94 HB - V-0HB - V-0Grade Count:9
Oxygen Index 22.0 - 37.0 %22.0 - 37.0 %Average value: 27.0 % Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
Overview of materials for Polystyrene, Molded, Unreinforced
Overview of materials for Polyimide

O4460a / 89092

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.