MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corning 1724 Aluminosilicate Crushed/Powdered Glass
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.64 g/cc0.0954 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.40 µm/m-°C
@Temperature 0.000 - 300 °C
2.44 µin/in-°F
@Temperature 32.0 - 572 °F
Softening Point 926 °C1700 °F
Annealing Point 726 °C1340 °F
Strain Point 674 °C1250 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Schott Glass 8240 Alkaline Earth Aluminosilicate Glass
Esstech V-115-1104 Aluminosilicate Glass-Ceramic
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere

CCORNG02 / 734

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.