System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere
Categories:
Ceramic
;
Glass
;
Other Engineering Material
;
Additive/Filler for Polymer
Material Notes:
Fine particle white spheres developed as filler for paints, coatings and films.
Information provided by Potters Industries.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.800
g/cc
0.0289
lb/in³
Bulk Density measured via tamp density method after 1500 tamps
1.80
g/cc
0.0650
lb/in³
Effective Density measured in SAE 20 motor oil using Gardner cup
Density
2.10
g/cc
0.0759
lb/in³
True Density measured via nitrogen gas displacement pycnometer
Brightness
>= 95 %
>= 95 %
Hunter Whiteness
Oil Absorption
0.22 %
0.22 %
By mass (g oil/g spheres)
Particle Size
>=
3.0
µm
>=
3.0
µm
D10
5.0
µm
5.0
µm
Mean, measured using laser light scattering
5.0
µm
5.0
µm
D50
<=
20
µm
<=
20
µm
D90
<=
25
µm
<=
25
µm
D97
Mechanical Properties
Metric
English
Comments
Hardness, Mohs
6.0
6.0
Compressive Strength
>=
414
MPa
>=
60000
psi
Descriptive Properties
Color
White
Shape
spherical
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Corning 1724 Aluminosilicate Crushed/Powdered Glass
Esstech V-115-1104 Aluminosilicate Glass-Ceramic
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Schott Glass 8240 Alkaline Earth Aluminosilicate Glass
CPOT9932 / 161922
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.