MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere
Categories: Ceramic; Glass; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fine particle white spheres developed as filler for paints, coatings and films.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.800 g/ccBulk Density measured via tamp density method after 1500 tamps
 1.80 g/ccEffective Density measured in SAE 20 motor oil using Gardner cup
Density 2.10 g/ccTrue Density measured via nitrogen gas displacement pycnometer
Brightness >= 95 %Hunter Whiteness
Oil Absorption 0.22 %By mass (g oil/g spheres)
Particle Size >= 3.0 µmD10
 5.0 µmMean, measured using laser light scattering
 5.0 µmD50
 <= 20 µmD90
 <= 25 µmD97
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 6.0
Compressive Strength >= 60000 psi
 
Descriptive Properties
ColorWhite
Shapespherical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Corning 1724 Aluminosilicate Crushed/Powdered Glass
Esstech V-115-1104 Aluminosilicate Glass-Ceramic
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Schott Glass 8240 Alkaline Earth Aluminosilicate Glass

CPOT9932 / 161922

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.