MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for T S10000 Series Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T S10000 Series Stainless Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "T S10000 Series Stainless Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 - 7.82 g/cc0.278 - 0.283 lb/in³Average value: 7.77 g/cc Grade Count:73
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 258 - 567258 - 567Average value: 377 Grade Count:37
Hardness, Knoop 265 - 631265 - 631Average value: 408 Grade Count:36
Hardness, Rockwell B 88.5 - 10488.5 - 104Average value: 99.0 Grade Count:17
Hardness, Rockwell C 21.5 - 55.521.5 - 55.5Average value: 38.9 Grade Count:49
Hardness, Vickers 153 - 604153 - 604Average value: 382 Grade Count:38
Tensile Strength, Ultimate 848 - 2520 MPa123000 - 365000 psiAverage value: 1270 MPa Grade Count:69
Tensile Strength, Yield 421 - 2100 MPa61100 - 305000 psiAverage value: 1100 MPa Grade Count:68
Elongation at Break 0.000 - 28.5 %0.000 - 28.5 %Average value: 12.2 % Grade Count:68
Reduction of Area 10.0 - 66.0 %10.0 - 66.0 %Average value: 47.4 % Grade Count:13
Modulus of Elasticity 77.0 - 230 GPa11200 - 33400 ksiAverage value: 197 GPa Grade Count:62
Poissons Ratio 0.2720.272Average value: 0.272 Grade Count:7
Machinability 35.0 - 40.0 %35.0 - 40.0 %Average value: 37.5 % Grade Count:7
Shear Modulus 77.4 GPa11200 ksiAverage value: 77.4 GPa Grade Count:7
Charpy Impact 10.0 - 236 J7.38 - 174 ft-lbAverage value: 69.1 J Grade Count:31
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000770 - 0.000100 ohm-cm0.0000770 - 0.000100 ohm-cmAverage value: 0.0000828 ohm-cm Grade Count:41
Magnetic Permeability 95.095.0Average value: 95.0 Grade Count:18
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.50 - 13.0 µm/m-°C5.28 - 7.22 µin/in-°FAverage value: 11.0 µm/m-°C Grade Count:65
Specific Heat Capacity 0.419 - 0.460 J/g-°C0.100 - 0.110 BTU/lb-°FAverage value: 0.437 J/g-°C Grade Count:41
Melting Point 1400 - 1470 °C2550 - 2680 °FAverage value: 1430 °C Grade Count:38
Solidus 1400 - 1410 °C2550 - 2560 °FAverage value: 1400 °C Grade Count:38
Liquidus 1440 - 1470 °C2620 - 2680 °FAverage value: 1450 °C Grade Count:38
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.750 - 1.50 %0.750 - 1.50 %Average value: 1.13 % Grade Count:42
Carbon, C 0.0400 - 0.0900 %0.0400 - 0.0900 %Average value: 0.0619 % Grade Count:74
Chromium, Cr 12.3 - 19.5 %12.3 - 19.5 %Average value: 14.8 % Grade Count:74
Copper, Cu 3.00 - 5.00 %3.00 - 5.00 %Average value: 3.59 % Grade Count:31
Iron, Fe 70.6 - 79.6 %70.6 - 79.6 %Average value: 74.2 % Grade Count:74
Manganese, Mn 0.100 - 2.50 %0.100 - 2.50 %Average value: 0.843 % Grade Count:71
Molybdenum, Mo 1.50 - 3.00 %1.50 - 3.00 %Average value: 2.39 % Grade Count:35
Nb + Ta 0.150 - 0.450 %0.150 - 0.450 %Average value: 0.300 % Grade Count:25
Nickel, Ni 3.00 - 8.75 %3.00 - 8.75 %Average value: 6.44 % Grade Count:73
Niobium, Nb (Columbium, Cb) 0.300 - 0.450 %0.300 - 0.450 %Average value: 0.381 % Grade Count:13
Nitrogen, N 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:7
Phosphorus, P 0.0100 - 0.0700 %0.0100 - 0.0700 %Average value: 0.0270 % Grade Count:68
Silicon, Si 0.100 - 1.00 %0.100 - 1.00 %Average value: 0.828 % Grade Count:68
Sulfur, S 0.00800 - 0.150 %0.00800 - 0.150 %Average value: 0.0226 % Grade Count:68
Tantalum, Ta 0.450 %0.450 %Average value: 0.450 % Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for T 300 Series Stainless Steel
Overview of materials for T 400 Series Stainless Steel
Overview of materials for Precipitation Hardening Stainless
303 Stainless Steel, annealed
Overview of materials for T 600 Series Stainless Steel

M01027 / 81738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.