MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for T 400 Series Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "T 400 Series Stainless Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.13 - 7.87 g/cc0.221 - 0.284 lb/in³Average value: 7.72 g/cc Grade Count:309
Particle Size 6.70 - 12.0 µm6.70 - 12.0 µmAverage value: 9.27 µm Grade Count:24
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 131 - 594131 - 594Average value: 254 Grade Count:106
Hardness, Knoop 146 - 662146 - 662Average value: 293 Grade Count:70
Hardness, Rockwell A 51.1 - 56.451.1 - 56.4Average value: 53.0 Grade Count:6
Hardness, Rockwell B 42.0 - 13042.0 - 130Average value: 85.6 Grade Count:152
Hardness, Rockwell C 10.0 - 59.010.0 - 59.0Average value: 40.5 Grade Count:106
Hardness, Vickers 140 - 1100140 - 1100Average value: 337 Grade Count:74
Tensile Strength, Ultimate 280 - 2070 MPa40600 - 300000 psiAverage value: 861 MPa Grade Count:292
Tensile Strength, Yield 165 - 1900 MPa23900 - 276000 psiAverage value: 681 MPa Grade Count:261
Elongation at Break 1.00 - 46.0 %1.00 - 46.0 %Average value: 19.6 % Grade Count:247
Elongation at Yield 2.00 - 40.0 %2.00 - 40.0 %Average value: 15.5 % Grade Count:7
Reduction of Area 0.500 - 77.0 %0.500 - 77.0 %Average value: 47.7 % Grade Count:58
Modulus of Elasticity 199 - 215 GPa28900 - 31200 ksiAverage value: 200 GPa Grade Count:262
Notched Tensile Strength 793 - 2070 MPa115000 - 300000 psiAverage value: 1740 MPa Grade Count:8
Bulk Modulus 166 GPa24100 ksiAverage value: 166 GPa Grade Count:4
Poissons Ratio 0.200 - 0.3800.200 - 0.380Average value: 0.250 Grade Count:63
Fatigue Strength 85.0 - 772 MPa12300 - 112000 psiAverage value: 389 MPa Grade Count:23
Shear Modulus 62.1 - 83.9 GPa9000 - 12200 ksiAverage value: 80.2 GPa Grade Count:64
Izod Impact 16.3 - 122 J12.0 - 90.0 ft-lbAverage value: 71.2 J Grade Count:28
Izod Impact Unnotched 54.2 - 122 J40.0 - 90.0 ft-lbAverage value: 78.0 J Grade Count:3
Charpy Impact 7.00 - 133 J5.16 - 98.1 ft-lbAverage value: 51.6 J Grade Count:32
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000236 - 0.000120 ohm-cm0.0000236 - 0.000120 ohm-cmAverage value: 0.0000612 ohm-cm Grade Count:255
Magnetic Permeability 400 - 2200400 - 2200Average value: 885 Grade Count:51
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.20 - 16.8 µm/m-°C5.11 - 9.33 µin/in-°FAverage value: 11.5 µm/m-°C Grade Count:247
Specific Heat Capacity 0.427 - 0.477 J/g-°C0.102 - 0.114 BTU/lb-°FAverage value: 0.461 J/g-°C Grade Count:197
Thermal Conductivity 15.0 - 27.0 W/m-K104 - 187 BTU-in/hr-ft²-°FAverage value: 24.0 W/m-K Grade Count:76
Melting Point 1370 - 1530 °C2500 - 2790 °FAverage value: 1480 °C Grade Count:195
Solidus 1370 - 1480 °C2500 - 2700 °FAverage value: 1450 °C Grade Count:188
Liquidus 1480 - 1530 °C2700 - 2790 °FAverage value: 1510 °C Grade Count:188
Maximum Service Temperature, Air 620 - 1100 °C1150 - 2000 °FAverage value: 772 °C Grade Count:93
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 593 - 999 °C1100 - 1830 °FAverage value: 796 °C Grade Count:3
Hot-Working Temperature 750 - 1200 °C1380 - 2190 °FAverage value: 1010 °C Grade Count:3
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0100 - 4.00 %0.0100 - 4.00 %Average value: 0.632 % Grade Count:20
Carbon, C 0.00900 - 1.60 %0.00900 - 1.60 %Average value: 0.212 % Grade Count:354
Chromium, Cr 10.0 - 51.0 %10.0 - 51.0 %Average value: 14.9 % Grade Count:355
Copper, Cu 0.500 - 2.50 %0.500 - 2.50 %Average value: 1.56 % Grade Count:16
Iron, Fe 47.1 - 89.1 %47.1 - 89.1 %Average value: 82.3 % Grade Count:355
Manganese, Mn 0.0350 - 2.00 %0.0350 - 2.00 %Average value: 0.969 % Grade Count:349
Molybdenum, Mo 0.0270 - 4.00 %0.0270 - 4.00 %Average value: 0.788 % Grade Count:144
Nb + Ta 0.100 - 0.600 %0.100 - 0.600 %Average value: 0.457 % Grade Count:23
Nickel, Ni 0.230 - 10.5 %0.230 - 10.5 %Average value: 1.48 % Grade Count:149
Niobium, Nb (Columbium, Cb) 0.150 - 1.50 %0.150 - 1.50 %Average value: 0.518 % Grade Count:25
Nitrogen, N 0.0120 - 0.100 %0.0120 - 0.100 %Average value: 0.0239 % Grade Count:26
Phosphorus, P 0.0100 - 0.400 %0.0100 - 0.400 %Average value: 0.0394 % Grade Count:299
Potassium, K 0.0600 %0.0600 %Average value: 0.0600 % Grade Count:8
Selenium, Se 0.150 %0.150 %Average value: 0.150 % Grade Count:15
Silicon, Si 0.0500 - 1.80 %0.0500 - 1.80 %Average value: 0.903 % Grade Count:348
Sulfur, S 0.00100 - 4.00 %0.00100 - 4.00 %Average value: 0.0472 % Grade Count:312
Tantalum, Ta 0.500 %0.500 %Average value: 0.500 % Grade Count:5
Titanium, Ti 0.00500 - 1.40 %0.00500 - 1.40 %Average value: 0.480 % Grade Count:38
Tungsten, W 0.750 - 3.00 %0.750 - 3.00 %Average value: 1.30 % Grade Count:20
Vanadium, V 0.150 - 0.400 %0.150 - 0.400 %Average value: 0.241 % Grade Count:20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for T 300 Series Stainless Steel
Overview of materials for Stainless Steel
Overview of materials for T 600 Series Stainless Steel
Overview of materials for T S10000 Series Stainless Steel
Overview of materials for Precipitation Hardening Stainless

M01025 / 81736

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.