MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® L 25H FWA black 9225 PA12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product Description: Grilamid L 25 H FWA black 9225 is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA black 9225 is designed for technical injection moulded components, and is in particular suitable for parts with medium or high wall thicknesses. The maximum thickness can largely exceed 15 mm.
  • high impact strength
  • high elongation
  • very low moisture absorption
  • good chemical resistance
  • high melt viscosity
  • easy processing
  • low density
Application examples: The particular stabilisation package of Grilamid L 25 H FWA black 9225 allows the use in direct contact with potable water and foodstuff.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Water Absorption 1.5 %1.5 %ISO 62
Moisture Absorption 0.700 %0.700 %ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070conditioned, 15s; ISO 868
Tensile Strength, Yield 40.0 MPa5800 psi
Elongation at Break >= 50 %>= 50 %conditioned; ISO 527-1/-2
Elongation at Yield 12 %12 %conditioned; ISO 527-1/-2
Tensile Modulus 1.10 GPa160 ksiconditioned; ISO 527-1/-2
Charpy Impact Unnotched NBNBconditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²conditioned; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Strength 32.0 kV/mm813 kV/inconditioned; IEC 60243-1
Comparative Tracking Index 600 V600 Vconditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C77.8 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C212 - 248 °Flong term; EMS
 150 °C302 °Fshort term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
Food contactEU Requirements
 NSF 51
FormGranules
Industry & Consumer goodsHeating systems
 Housewares
 Sanitary, water and gas supply
ProcessingInjection Molding
Product AttributesHydrolysis resistant
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)
Water ContactACS
 DVGW W270
 KTW
 NSF 61
 WRAS

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsamid® AESN BLACK P202 T6L PA12-I
EMS-Grivory Grilamid® L 20H FWA black 9225 PA12
EMS-Grivory Grilamid® L 20 HL black 9563 PA12
EMS-Grivory Grilamid® L 16 W 20 black 9995 PA12
EMS-Grivory Grilamid® L 20 H FR PA12 FR

PGRH057 / 156766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.