MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese AT 234 Low Density Polyethylene (LDPE)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: AT 234 is a black homopolymer compound recommended for higher pressure series pipe applications such as municipal water service pipe. It has an ASTM D1248 classification of IC3-P14. Additives:

Applications: Tubes & Pipes

Information provided by Celanese Corporation.

Key Words: higher pressure series pipe applications such as municipal water service pipe
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.929 g/cc0.0336 lb/in³AT Plastics PTM-03
Carbon Black Loading 2.2 %2.2 %Deviation from Target; ASTM D1603
Melt Flow 1.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 14.0 MPa2030 psiType IV (50 mm/min); ASTM D638
Tensile Strength, Ultimate 2.80 MPa406 psiCertified Design Strength; CSA B137
Elongation at Break 530 %530 %Type IV (50 mm/min); ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 113 °C235 °FDSC; ASTM D3417
Vicat Softening Point 97.0 °C207 °FASTM D1525
Brittleness Temperature -79.0 °C-110 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 205°C (400°F) temper, 25 mm (1 in.) round
Celanese AT 253 Low Density Polyethylene (LDPE)
Mitsubishi Chemical Advanced Materials Proteus™ LDPE Low Density Polyethylene
Overview of materials for Low Density Polyethylene (LDPE), Film Grade

PATEVB77 / 26033

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.