MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene® LD-702 High EVA Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and toughness.

Applications: Pallet stretch wrap; Heat seal layer in coextruded or laminated structures; Liquid packaging; Profile extrusions; Compounding; Frozen food bags.

Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.943 g/cc0.0341 lb/in³Exxon Method
Environmental Stress Crack Resistance >= 500 hour>= 500 hourF50, Condition A; ASTM D1693
Melt Flow 0.30 g/10 min0.30 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383ASTM D2240
Hardness, Shore D 3333ASTM D2240
Tensile Strength, Ultimate 17.0 MPa2470 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus, 1% Secant 83.0 MPa12000 psiASTM D790
Tensile Impact Strength 773 kJ/m²368 ft-lb/in²23°C; ASTM D-1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 92.0 °C198 °FExxon Method
Vicat Softening Point 77.0 °C171 °F1000g; ASTM D-1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Polyvinyl Fluoride (PVF) Film
ExxonMobil EVA 25028.CM Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
ExxonMobil Escorene™ Ultra LD 720.01 Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
ExxonMobil Escorene® LD 701.ID Blown Film Resin
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations

PEXCDL / 37861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.