MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

IRPC Polimaxx Pentfoam 155E Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: General: Pentfoam 155E is a self extinguising grad expandable polystyrene containing pentate as blowing agent

Applications: Pentfoam 155E is particularly well suited for the manufacture of low density self extinguishing eps insulation boards and panels. This grade is also widely used for the production of low density decoration products, and drainage boards.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0120 - 0.0130 g/cc0.000434 - 0.000470 lb/in³
 0.0120 - 0.0200 g/cc0.000434 - 0.000723 lb/in³molding density range
Bead Size 1.60 - 2.24 mm0.0630 - 0.0882 in
Maximum Moisture Content 0.200.20
 
Chemical PropertiesMetricEnglishComments
Blowing Agent Content >= 5.9 %>= 5.9 %
 
Mechanical PropertiesMetricEnglishComments
K Factor (Wear Factor) 55 - 5955 - 59

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical R160 EPS, Flame Retardant
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
LG Chemical R320 EPS, Flame Retardant
Sekisui PIOCELAN SP-50D Moldable Polymer Foam
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer

PIRPC015 / 83992

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.