MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Orthtek WF components work well as metal replacements due to Orthtek’s high strength, low weight, corrosion resistance, and dimensional stability. Orthtek WF is recommended for applications such as nail guides and retractors where radiolucentcy and autoclaving are required.

Applications:

  • Medical Trauma – External fixation and targeting devices
  • Medical Orthopedic – Reconstructive components, retractors, spine instrumentation and surgical instrumentation

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc1.54 g/ccASTM D792
Filler Content 50.0 %50.0 %Fiber Volume
Water Absorption 0.050 %0.050 %at 212°F (100°C); ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 627 MPa91000 psiASTM D3039
Elongation at Break 1.0 %1.0 %ASTM D3039
Tensile Modulus 60.0 GPa8700 ksiASTM D3039
Flexural Strength 827 MPa120000 psiASTM D790
Flexural Modulus 48.3 GPa7000 ksiASTM D790
Compressive Strength 572 MPa83000 psiASTM D695
Compressive Modulus 55.2 GPa8000 ksiASTM D695
 
Descriptive Properties
ColorBlack
Fiber Orientation[0/90]s
Fiber Tow Size3K

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber
Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
ASTM A228 Steel (UNS K08500)

PGREEN76 / 42370

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.