Envalior Durethan® BKV 30 N1 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 30% Glass Fiber Filled
Material Notes:
PA 6, 30% glass fibers, injection molding, flame retardant
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.58
g/cc
0.0571
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
1.5 %
1.5 %
50% RH; ISO 62
Water Absorption at Saturation
5.1 %
5.1 %
IOS 62
Linear Mold Shrinkage, Flow
0.0022
cm/cm
0.0022
in/in
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0060
cm/cm
0.0060
in/in
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
80.0
MPa
11600
psi
5 mm/min; ISO 527-1,-2
Tensile Strength, Yield
80.0
MPa
11600
psi
50 mm/min; ISO 527-1,-2
Elongation at Break
3.6 %
3.6 %
5 mm/min; ISO 527-1,-2
4.0 %
4.0 %
Nominal, 50 mm/min; ISO 527-1,-2
Elongation at Yield
3.5 %
3.5 %
50 mm/min; ISO 527-1,-2
Tensile Modulus
6.50
GPa
943
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
145
MPa
21000
psi
2 mm/min; ISO 178-A
Flexural Modulus
7.50
GPa
1090
ksi
2 mm/min; ISO 178-A
Flexural Strain at Break
3.5 %
3.5 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
<=
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)
45.0
kJ/m²
21.4
ft-lb/in²
ISO 180-1U
Charpy Impact Unnotched
4.50
J/cm²
@Temperature -30.0 °C
21.4
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
5.50
J/cm²
@Temperature 23.0 °C
26.2
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched
<=
1.00
J/cm²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
<=
1.00
J/cm²
@Temperature -40.0 °C
<=
4.76
ft-lb/in²
@Temperature -40.0 °F
ISO 179 1eA
1.20
J/cm²
@Temperature 23.0 °C
5.71
ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Puncture Energy
9.00
J
@Temperature 23.0 °C
6.64
ft-lb
@Temperature 73.4 °F
ISO 6603-2
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+11
ohm-cm
1.00e+11
ohm-cm
IEC 60093
Surface Resistance
1.00e+14
ohm
1.00e+14
ohm
IEC 60093
Dielectric Constant
4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
IEC 60250
8.0
@Frequency 100 Hz
8.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength
27.0
kV/mm
@Thickness 1.00 mm
686
kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor
0.045
@Frequency 1e+6 Hz
0.045
@Frequency 1e+6 Hz
IEC 60250
0.13
@Frequency 100 Hz
0.13
@Frequency 100 Hz
IEC 60250
Thermal Properties
Metric
English
Comments
Melting Point
225
°C
437
°F
225
°C
437
°F
Processing Properties
Metric
English
Comments
Melt Temperature
250
°C
482
°F
injection molding
240
-
260
°C
464
-
500
°F
Mold Temperature
80.0
°C
176
°F
injection molding
80.0
-
100
°C
176
-
212
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Envalior Durethan® BKV 30 N1 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Celanese CoolPoly® D5502 Thermally Conductive Liquid Crystalline Polymer
Polyglyconate
Overview of materials for Cellulose Acetate, Molded
PLANW9393 / 208220
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.