MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.

Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.

Uses: Tube/Hose and Sheet Extrusion, Wire/Cable

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
 1.15 g/cc1.15 g/ccPVC (80)/CP80AS2(20)
 1.15 g/cc1.15 g/ccPVC (70)/CP80AS2(30)
 1.15 g/cc1.15 g/ccPVC (50)/CP80AS2(50)
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262PVC (80)/CP80AS2(20)
 6363PVC (70)/CP80AS2(30)
 6565PVC (50)/CP80AS2(50)
 81
@Time 5.00 sec
81
@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 15.9 MPa2310 psiPVC (80)/CP80AS2(20)
 18.6 MPa2700 psiPVC (70)/CP80AS2(30)
 24.1 MPa3500 psiPVC (50)/CP80AS2(50)
Tensile Strength, Ultimate 27.6 MPa4000 psiASTM D412
Elongation at Break 470 %470 %ASTM D412
 540 %540 %PVC (80)/CP80AS2(20)
 580 %580 %PVC (70)/CP80AS2(30)
 665 %665 %PVC (50)/CP80AS2(50)
100% Modulus 3.90 MPa
@Strain 100 %
566 psi
@Strain 100 %
ASTM D412
300% Modulus 8.40 MPa
@Strain 300 %
1220 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.00383 GPa0.555 ksiPVC (80)/CP80AS2(20)
 0.00434 GPa0.630 ksiPVC (70)/CP80AS2(30)
 0.00579 GPa0.840 ksiPVC (50)/CP80AS2(50)
Tear Strength 5.43 kN/m31.0 pliTrouser, PVC (80)/CP80AS2(20)
 7.01 kN/m40.0 pliTrouser, PVC (70)/CP80AS2(30)
 11.7 kN/m67.0 pliTrouser, PVC (50)/CP80AS2(50)
 21.9 kN/m125 pliTrouser; ASTM D470
Graves Tear Strength 29.8 kN/m170 pliPVC (80)/CP80AS2(20)
 33.3 kN/m190 pliPVC (70)/CP80AS2(30)
 47.3 kN/m270 pliPVC (50)/CP80AS2(50)
 63.1 kN/m360 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 8686PVC (50)/CP80AS2(50)
 128128PVC (70)/CP80AS2(30)
 146146PVC (80)/CP80AS2(20)
 14
@Load 1.00 kg
14
@Load 2.20 lb
H-18 wheel; ASTM D3389
Abrasion 8383[mm3], PVC (50)/CP80AS2(50)
 126126[mm3], PVC (70)/CP80AS2(30)
 148148[mm3], PVC (80)/CP80AS2(20)
Compression Set 13 %13 %PVC (80)/CP80AS2(20)
 16 %16 %PVC (70)/CP80AS2(30)
 19 %19 %PVC (50)/CP80AS2(50)
Tensile Set 14 %14 %PVC (50)/CP80AS2(50)
 16 %16 %PVC (70)/CP80AS2(30)
 19 %19 %PVC (80)/CP80AS2(20)
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 °C284 °FDSC
Glass Transition Temp, Tg -30.0 °C-22.0 °FDSC
 
Processing PropertiesMetricEnglishComments
Zone 1 170 °C338 °FExtrusion
Zone 2 175 °C347 °FExtrusion
Zone 3 180 °C356 °FExtrusion
Zone 4 180 °C356 °FExtrusion
Adapter Temperature 180 °C356 °F5, Extrusion
Die Temperature 180 °C356 °F6, Zone 1, Extrusion
 180 °C356 °FZone 2, Extrusion
Drying Temperature 150 °C302 °Fovernight
Dew Point -40.0 °C-40.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 890 AN TPUR
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane
Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane
Lubrizol Estane® ALR E72A Thermoplastic Polyurethane
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane

PNOVEON585 / 121476

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.