MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Elastollan® 890 AN TPUR
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilience performance.

Typical Applications: Polyester based for transparent films.

Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°C

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183-1-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494ISO 868
Tensile Strength 50.0 MPa7250 psiISO 37
Tensile Strength, Yield 5.70 MPa827 psi20% Strain; ISO 37
Elongation at Break 550 %550 %ISO 37
100% Modulus 10.0 MPa
@Strain 100 %
1450 psi
@Strain 100 %
ISO 37
300% Modulus 22.5 MPa
@Strain 300 %
3260 psi
@Strain 300 %
ISO 37
Charpy Impact, Notched  20.0 J/cm²
@Temperature -30.0 °C
95.2 ft-lb/in²
@Temperature -22.0 °F
DIN ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DIN ISO 179
Tear Strength 120 kN/m685 pliDIN ISO 34-1/Bb
Abrasion 4545[mm3; ISO 4649
Compression Set  32 %
@Temperature 23.0 °C
32 %
@Temperature 73.4 °F
DIN EN ISO 815
 43 %
@Temperature 70.0 °C
43 %
@Temperature 158 °F
DIN EN ISO 815
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 220 °C347 - 428 °FExtrusion
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °F
 
Descriptive Properties
Commercial StatusNorth America
Primary Processing TechniqueExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® B 90 A TPUR
Lubrizol Estane® ALR E72A Thermoplastic Polyurethane
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane
Lubrizol Estane® ALR G500 Water Absorbent Thermoplastic Polyurethane

PBASG0541 / 132174

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.