MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Koattro DP 0400M Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polybutene

Material Notes: Koattro is a novel family of high-molecular-weight plastomers. Polybutene-1 grade Koattro DP 0400M is a semi-crystalline homopolymer, which can  be used where creep, environmental stress crack resistance and elevated temperature performance are key requirements. This polymer is highly compatible with polypropylene due to its similar molecular structure. It is less compatible in blends with polyethylene but it is still easily dispersible. Its relative slow crystallization kinetics allows for an excellent wetting behavior. Besides its high shear sensitive flow behavior it remains easily dispersible, also in even more incompatible polymers like thermoplastic elastomers. Applications: Color Concentrates, Products for Use in Property Modification.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.915 g/cc0.0331 lb/in³ISO 1183-1
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 29.0 MPa4210 psiISO 8986-2
Elongation at Break 300 %300 %ISO 8986-2
Flexural Modulus 0.450 GPa65.3 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 114 °C237 °FTm2; ISO 11357-3
 126 °C259 °FTm1; ISO 11357-3
 
Descriptive Properties
Processing MethodMelt Blown, Spunbond, Staple Fiber

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Toppyl PB 0110M Polybutene
LyondellBasell Toppyl PB 8220M Polybutene
LyondellBasell Koattro PB 0300M Polymer
LyondellBasell Alathon® M5370WC High Density Polyethylene
LyondellBasell Akoalit PB 4237 grey Polyolefin

PEQT7602 / 219239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.