MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Toppyl PB 8220M Polybutene
Categories: Polymer; Film; Thermoplastic; Polybutene

Material Notes: Polybutene-1 (PB-1) grade Toppyl PB 8220M is a random copolymer of butene-1 with medium ethylene content. This grade is highly compatible with polypropylene due to its similar molecular structure, and it is used to modify the sealing behavior of PP based films: a typical example is its use to reduce the seal initiation temperature of BOPP sealing layers. The relatively slow kinetics of crystallization allow an excellent wetting behavior. Toppyl PB 8220M highly shear-sensitive flow behavior means that it remains easily dispersible also in even more incompatible polymers like thermoplastic elastomers. Toppyl PB 8220M can also be used in seal-peel application. Compared with Toppyl PB 8640M or Toppyl PB 8340M, in blown film seal-peel Toppyl PB 8220M provides better optical properties (haze and clarity) but with narrow sealing window. Applications: Bags & Pouches, Food Packaging Film, Lamination Film, Peelable Film, Secondary Packaging, Specialty Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.901 g/cc0.0326 lb/in³ISO 1183-1
Melt Flow  2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 7.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 46 g/10 min
@Load 10.0 kg,
Temperature 190 °C
46 g/10 min
@Load 22.0 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 32.0 MPa4640 psiISO 8986-2
Elongation at Break 300 %300 %ISO 8986-2
Flexural Modulus 0.140 GPa20.3 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 85.0 °C185 °FTm2; ISO 11357-3
 97.0 °C207 °FTm1; ISO 11357-3
 
Descriptive Properties
Processing MethodBlown Film, BOPP, Cast Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borstar® FB4230 LLDPE for Film
M. Holland Company LD800 LDPE
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Baystar™ Lumicene® mPE M 2710 EP Metallocene Medium Density Polyethylene Film Resin
LyondellBasell Toppyl PB 8340M Polybutene

PEQT8588 / 220223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.