System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Zytel® BM7300THS BK317 PA6-HI
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Impact Grade
Material Notes:
Toughened, Heat Stabilized, Polyamide 6 Developed for Blow Molding
Former DuPont product acquired by Celanese in 2022.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.09
g/cc
0.0394
lb/in³
DAM; ISO 1183
Viscosity
440000
cP
@Shear Rate 1000 1/s,
Temperature 280 °C
440000
cP
@Shear Rate 1000 1/s,
Temperature 536 °F
Melt; ISO 11443
Linear Mold Shrinkage, Flow
0.011
cm/cm
0.011
in/in
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.011
cm/cm
0.011
in/in
DAM; ISO 294-4, 2577
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
60.0
MPa
8700
psi
DAM; ISO 527-1/-2
Elongation at Break
>= 50 %
>= 50 %
Nominal; DAM; ISO 527-1/-2
Elongation at Yield
4.2 %
4.2 %
DAM; ISO 527-1/-2
Tensile Modulus
0.600
GPa
87.0
ksi
50% RH; ISO 527-1/-2
2.20
GPa
319
ksi
DAM; ISO 527-1/-2
Poissons Ratio
0.39
0.39
DAM
0.47
0.47
50% RH
Izod Impact, Notched (ISO)
18.0
kJ/m²
@Temperature -30.0 °C
8.57
ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
20.0
kJ/m²
@Temperature -30.0 °C
9.52
ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
38.0
kJ/m²
@Temperature 23.0 °C
18.1
ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
120
kJ/m²
@Temperature 23.0 °C
57.1
ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched
1.40
J/cm²
@Temperature -40.0 °C
6.66
ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
1.50
J/cm²
@Temperature -40.0 °C
7.14
ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
2.10
J/cm²
@Temperature -30.0 °C
9.99
ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
2.20
J/cm²
@Temperature -30.0 °C
10.5
ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
4.50
J/cm²
@Temperature 23.0 °C
21.4
ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
15.0
J/cm²
@Temperature 23.0 °C
71.4
ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Thermal Properties
Metric
English
Comments
Melting Point
220
°C
428
°F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
100
°C
212
°F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
52.0
°C
126
°F
DAM; ISO 75-1/-2
Glass Transition Temp, Tg
10.0
°C
50.0
°F
10°C/min; 50% RH; ISO 11357-1/-2
60.0
°C
140
°F
10°C/min; DAM; ISO 11357-1/-2
Flame Spread
<=
80.0
mm/min
@Thickness 1.00 mm
<=
3.15
in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Processing Properties
Metric
English
Comments
Melt Temperature
235
-
250
°C
455
-
482
°F
Range, Extrusion
255
-
265
°C
491
-
509
°F
Range, Blow Molding
260
°C
500
°F
Optimum, Blow Molding
270
°C
518
°F
Optimum, Injection
260
-
280
°C
500
-
536
°F
Range, Injection
Mold Temperature
70.0
°C
158
°F
Optimum, Injection
50.0
-
100
°C
122
-
212
°F
Injection
90.0
°C
194
°F
Optimum, Blow Molding
80.0
-
110
°C
176
-
230
°F
Range, Blow Molding
Drying Temperature
80.0
°C
176
°F
Injection
80.0
°C
176
°F
Extrusion
110
-
120
°C
230
-
248
°F
Blow Molding
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Injection, Dehumidified Dryer
4.00
-
6.00
hour
4.00
-
6.00
hour
Blow Molding, Dehumidified Dryer
4.00
-
6.00
hour
4.00
-
6.00
hour
Extrusion, Dehumidified Dryer
Moisture Content
<= 0.030 %
<= 0.030 %
Blow Molding
<= 0.060 %
<= 0.060 %
Extrusion
<= 0.20 %
<= 0.20 %
Injection
Hold Pressure
50.0
-
100
MPa
7250
-
14500
psi
Range, Injection
Descriptive Properties
Drying Recommended
yes
Blow Molding
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
ISO designation
ISO 16396-PA6-I,,M1CG1HR,S14-020
Max. screw tangential speed (m/s)
0.2
Injection
Part Marking Code
>PA6-HI<
ISO 11469
Polymer
PA6-I
Processing Hold Pressure Time (s/mm)
3
Injection
Resin Identification
PA6-HI
ISO 1043
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Zytel® ST7301 BK356 PA6-HI
Celanese Zytel® 103FHSA NC010 PA66
Celanese Zytel® 151L NC010 PA612
Celanese Elvamide® 8061 PA6/66/610
Celanese Zytel® BM70G20HSLX BK537 PA66-IGF20
PDSX5386 / 198026
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.