MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® BM70G20HSLX BK537 PA66-IGF20
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: 20% Glass Reinforced, Heat Stabilized, Polyamide 66 Developed for Blow Molding

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³DAM; ISO 1183
Melt Density 1.07 g/cc
@Temperature 295 °C
0.0387 lb/in³
@Temperature 563 °F
Water Absorption 5.2 %
@Thickness 2.00 mm
5.2 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.60 %
@Thickness 2.00 mm
1.60 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity 330000 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
330000 cP
@Shear Rate 1000 1/s,
Temperature 536 °F
Melt; ISO 11443
Viscosity Number 155 cm³/g1.55 dl/gSulfuric acid 96%; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 225 MPa32600 psiH 961/30; DAM; ISO 2039-1
Tensile Strength at Break 75.0 MPa10900 psi50% RH; ISO 527-1/-2
 120 MPa17400 psiDAM; ISO 527-1/-2
Elongation at Break 4.0 %4.0 %DAM; ISO 527-1/-2
 13 %13 %50% RH; ISO 527-1/-2
Tensile Modulus 4.00 GPa580 ksi50% RH; ISO 527-1/-2
 6.50 GPa943 ksiDAM; ISO 527-1/-2
Flexural Strength 160 MPa23200 psiDS; DAM; ISO 178
Flexural Modulus 3.60 GPa522 ksi50% RH; ISO 178
 6.00 GPa870 ksiDAM; ISO 178
Poissons Ratio 0.350.35DAM
 0.360.3650% RH
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 16.0 kJ/m²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
@Temperature 23.0 °C
34.7 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.750 J/cm²
@Temperature -40.0 °C
3.57 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 3900 MPa566000 psi1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 3200 MPa464000 psi1000h; 50% RH; ISO 899-1
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 2.00 J/g-°C
@Temperature 295 °C
0.478 BTU/lb-°F
@Temperature 563 °F
Melt
Thermal Conductivity 0.200 W/m-K
@Temperature 295 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 563 °F
Melt
Melting Point 260 °C500 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 257 °C495 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 239 °C462 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 40.0 °C104 °F10°C/min; 50% RH; ISO 11357-1/-2
 65.0 °C149 °F10°C/min; DAM; ISO 11357-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 - 290 °C527 - 554 °FRange, Extrusion
 290 °C554 °FOptimum, Blow Molding
 295 °C563 °FOptimum, Injection
 285 - 305 °C545 - 581 °FRange, Blow Molding
 285 - 305 °C545 - 581 °FRange, Injection
Mold Temperature 50.0 - 100 °C122 - 212 °FInjection
 90.0 °C194 °FOptimum, Injection
 80.0 - 120 °C176 - 248 °FRange, Blow Molding
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
 80.0 °C176 °FExtrusion
 100 - 110 °C212 - 230 °FBlow Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 4.00 - 6.00 hour4.00 - 6.00 hourBlow Molding, Dehumidified Dryer
 4.00 - 6.00 hour4.00 - 6.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.050 %<= 0.050 %Blow Molding
 <= 0.060 %<= 0.060 %Extrusion
 <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
Drying RecommendedyesInjection
 Yes, if moisture content of resin exceeds recommended levelBlow Molding
FMVSS ClassSEISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66-I,GF20,M1CGH,S14-060
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66-IGF20<ISO 11469
PolymerPA66-GF20
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA66-IGF20ISO 1043
Swell ratio1.3Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR4275 BK316 TPC-ET
Techmer ES HiFill® PA6/6 GF20 L BK 20% Glass Filled
Celanese Zytel® BM7300THS BK317 PA6-HI
Celanese Zytel® 73G15HSL BK363 PA6-GF15
Celanese Zytel® 73G30HSL NC010 PA6-GF30

PDSX5385 / 198025

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.