MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade

Processing and Delivery Form: Pellets and Injection Molding

Special Characteristics: Improved stiffness

Information provided by Oxford Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Water Absorption at Saturation 0.030 %0.030 %ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 3.17 mm
0.0030 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 51.7 MPa7500 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 44.8 MPa6500 psiASTM D790
Flexural Modulus 1.90 GPa275 ksiASTM D790
Izod Impact, Notched 0.587 J/cm
@Thickness 3.17 mm
1.10 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C265 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 227 °C440 °F
Middle Barrel Temperature 238 °C460 °F
Front Barrel Temperature 241 °C465 °F
Nozzle Temperature 238 °C460 °F
Melt Temperature 241 °C465 °F
Mold Temperature 32.2 - 48.9 °C90.0 - 120 °F
Drying Temperature 76.7 °C170 °F
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced
Plastcom SLOVALEN PH 79 GF 20 Polypropylene Homopolymer, 20% Glass Fiber
Mocom (ALBIS) ALTECH® PP-H A 2020/750 GF20 Polypropylene Homopolymer, 20% Glass Fiber Reinforced
Niche Polymer PPHG20BK Homopolymer PP, 20% Glass Fiber Filled
Mocom (ALBIS) ALTECH® PP-B 2020/150 GF20 CP PP, 20% Glass Fiber Reinforced

POXF021 / 178451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.