MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALTECH® PP-H A 2020/750 GF20 Polypropylene Homopolymer, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Base Polymer: Polypropylene Homopolymer

Filler/Additive System: 20% glass fibers, chemically coupled

Special Features: Heat ageing stabilization, high stiffness

Market Segment: Electrical and Electronic, Building and Construction

Typical Applications: Injection molded parts

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Time 86400 sec
0.0030 - 0.0050 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Time 86400 sec
0.0040 - 0.0060 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527
Elongation at Break 3.4 %3.4 %ISO 527
Tensile Modulus 4.80 GPa696 ksiISO 527
Flexural Strength 105 MPa15200 psiISO 178
Flexural Modulus 3.90 GPa566 ksiISO 178
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 169 °C336 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 140 °C284 °FISO 75-1/-2
Vicat Softening Point 130 °C266 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 270 °C392 - 518 °FInjection molding
Mold Temperature 20.0 - 90.0 °C68.0 - 194 °FInjection molding
Drying Temperature  80.0 - 120 °C
@Time 7200 - 14400 sec
176 - 248 °F
@Time 2.00 - 4.00 hour
air circulating dryer
 80.0 - 120 °C
@Time 7200 - 10800 sec
176 - 248 °F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolypropylene Homopolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced
Niche Polymer PPHG20BK Homopolymer PP, 20% Glass Fiber Filled
Washington Penn Homopolymer Polypropylene 20% Glass Reinforced
Plastcom SLOVALEN PH 79 GF 20 Polypropylene Homopolymer, 20% Glass Fiber

PALBIS8852 / 242911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.