MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polygon Composites Polylube® MRP Versatile high load, low friction composite bearings
Categories: Polymer

Material Notes: The PolyLube® MRP bearing can withstand static loads of approximately 70,000 PSI and 30,000 PSI under dynamic loading. For dry running applications, the maximum speed is approximately 10 surface feet per minute. The typical average design pressure for high duty cycle applications is 10,000 PSI. This bearing’s operating temperature range is ±325°F. Maximum continuous operational surface temperature for the standard formulation is 325°F, depending upon load characteristics. The bearing has been heat stabilized at these temperatures, so that little dimensional change will occur in the bearing during operation. In a free state, the coefficient of expansion of the PolyLube MRP bearing is approximately 7 x 106 in/in/°F, similar to the coefficient of expansion for steel, and actually less than some metals.

Applications: PolyLube MRP bearings are the bearing of choice in highly loaded bearing joints where a life cycle of over 500,000 cycles is desired. Testing has shown this bearing has wear under 0.006" after 1.6 million cycles. Applications include material handling equipment, high duty cranes, earth-moving equipment, construction equipment, agriculture equipment and food processing systems. MRP bearings have extremely low absorption rates and are well designed for wet and submerged applications.

Information provided by Polygon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.87 g/cc1.87 g/cc
Water Absorption  0.12 %
@Time 7200 sec
0.12 %
@Time 2.00 hour
 0.16 %
@Time 86400 sec
0.16 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.3 MPa8750 psiAxial
 212.0 MPa30750 psiHoop
Modulus of Elasticity 6.69 GPa970 ksiRadial (wall)
 7.72 GPa1120 ksiTorsional Shear
 12.5 GPa1820 ksiAxial
 25.6 GPa3710 ksiHoop
Compressive Strength 0.1706 MPa24.75 psiAxial
 0.2116 MPa30.69 psiRadial (wall)
 0.212 MPa30.8 psiHoop
Compressive Modulus 0.483 GPa70.0 ksiUltimate
Poissons Ratio 0.210.21Uxy
 0.300.30Uxz
 0.420.42Uxy
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.64 µm/m-°C4.80 µin/in-°F
Thermal Conductivity 0.259 - 0.331 W/m-K1.80 - 2.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 163 °C325 °F
 
Descriptive Properties
Maximum Velocity10 SFM
Unit Load Limit30000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polygon Composites Polylube™ Fiber Series Epoxy Composite Bearings
Akro-Plastic Akrotek® PK-HM GF 30 (4709) PK Dry, 30% Glass Filled
Akro-Plastic Akrotek® PK-HM GF 30 (4709) PK Conditioned, 30% Glass Filled
Polykemi AB POLYblend 65H MA5 PC/ABS-blend, Low Friction
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Low friction, Low wear

PPOLYG04 / 184504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.